General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.47 g/cm³ Show Material materials with Densidad of 8.47 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Estricción | 20.0 °C | 18 % Show Material materials with Estricción of 18 % | |
650.0 °C | 29 % Show Material materials with Estricción of 29 % | ||
Límite elástico | 20.0 °C | 1330 MPa Show Material materials with Límite elástico of 1330 MPa | |
650.0 °C | 470 MPa Show Material materials with Límite elástico of 470 MPa | ||
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 20.0 °C | 1570 MPa Show Material materials with Resistencia a la tracción of 1570 MPa | |
650.0 °C | 572 MPa Show Material materials with Resistencia a la tracción of 572 MPa | ||
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 760.0 °C | 1.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.4E-5 1/K | The mentioned value is between 20°C and the mentioned temperature |
Chemical properties
Property | Value |
---|---|
Carbono | 0.55 % Show Material materials with Carbono of 0.55 % |
Cromo | 3.5 % Show Material materials with Cromo of 3.5 % |
Hierro | 81.55 - 100 % Show Material materials with Hierro of 81.55 - 100 % |
Manganeso | 0.2 % Show Material materials with Manganeso of 0.2 % |
Silicona | 0.2 % Show Material materials with Silicona of 0.2 % |
Wolframio | 14 % Show Material materials with Wolframio of 14 % |