Mecánica
Property | Temperature | Value |
---|---|---|
Estricción | 20.0 °C | 66 % Show Material materials with Estricción of 66 % |
760.0 °C | 31 % Show Material materials with Estricción of 31 % | |
Límite elástico | 20.0 °C | 360 MPa Show Material materials with Límite elástico of 360 MPa |
760.0 °C | 170 MPa Show Material materials with Límite elástico of 170 MPa | |
Resistencia a la tracción | 20.0 °C | 800 MPa Show Material materials with Resistencia a la tracción of 800 MPa |
760.0 °C | 320 MPa Show Material materials with Resistencia a la tracción of 320 MPa | |
Chemical properties
Property | Value |
---|---|
Carbono | 0.55 % Show Material materials with Carbono of 0.55 % |
Cromo | 21 % Show Material materials with Cromo of 21 % |
Hierro | 64.7 - 100 % Show Material materials with Hierro of 64.7 - 100 % |
Manganeso | 8.25 % Show Material materials with Manganeso of 8.25 % |
Nitrógeno | 0.45 % Show Material materials with Nitrógeno of 0.45 % |
Níquel | 2.8 % Show Material materials with Níquel of 2.8 % |
Silicona | 0.15 % Show Material materials with Silicona of 0.15 % |
Vanadio | 0.35 % Show Material materials with Vanadio of 0.35 % |
Wolframio | 1.75 % Show Material materials with Wolframio of 1.75 % |