Acero inoxidable austenítico
Alloy 24 / 1.4565 Solution annealed and quenchedSuministrada por:
Hempel Special MetalsAcero inoxidable austenítico
SEW 400 Grade X2CrNiMnMoNbN25-18-5-4 quenched (+Q)Acero inoxidable austenítico
EN 10090 Grade X50CrMnNiNbN21-9 solution heat-treated and precipitation hardened (+AT+P)Acero inoxidable austenítico
EN 10090 Grade X53CrMnNiN21-9 solution heat-treated and precipitation hardened (+AT+P)Acero inoxidable austenítico
DIN 17480 Grade X50CrMnNiNbN21-9 solution heat-treated and precipitation hardened (+AT+P)Acero inoxidable austenítico
DIN 17480 Grade X53CrMnNiN21-9 solution heat-treated and precipitation hardened (+AT+P)Acero inoxidable austenítico
ASTM A213 Grade S34565 Heat-TreatedAcero inoxidable austenítico
ASTM A240 Grade XM-17 Heat-TreatedAcero inoxidable austenítico
ASTM A240 Grade XM-18 Heat-TreatedAcero inoxidable austenítico
ASTM A240 Grade S34565 Heat-TreatedAcero inoxidable austenítico
ASTM A479 Grade S34565 AnnealedAcero inoxidable austenítico
ASTM A479 Grade XM-17 AnnealedAcero inoxidable austenítico
ASTM A479 Grade XM-18 AnnealedAcero inoxidable austenítico
SAE J775 Grade EV-8 For Mechanical Tests: ST+PAcero inoxidable austenítico
SAE J775 Grade XEV-F For Mechanical Tests: ST+PAcero inoxidable austenítico
SAE J775 Grade EV-13 For Mechanical Tests: ST+PAcero inoxidable martensítico
SEW 400 Grade X30CrMoN15-1 soft annealed (+A)Acero inoxidable austenítico
ASTM A276 Grade S28200 Annealed; Hot-Finished or Cold finished