General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel | ||||
Elongación | 11.6 % Show Material materials with Elongación of 11.6 % | Predicted Value, A80 | ||||
12.7 % Show Material materials with Elongación of 12.7 % | Predicted Value, A200 | |||||
13.9 % Show Material materials with Elongación of 13.9 % | Predicted Value, Transverse | |||||
17.9 % Show Material materials with Elongación of 17.9 % | Predicted Value, A5 | |||||
18.2 % Show Material materials with Elongación of 18.2 % | Predicted Value, A50 | |||||
18.6 % Show Material materials with Elongación of 18.6 % | Predicted Value, A80 Transverse | |||||
20 °C | 14 % Show Material materials with Elongación of 14 % | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
Estricción | 40.3 % Show Material materials with Estricción of 40.3 % | Predicted Value | ||||
44.6 % Show Material materials with Estricción of 44.6 % | Predicted Value, Transverse | |||||
Límite elástico | 307 MPa Show Material materials with Límite elástico of 307 MPa | Predicted Value, RP1 | ||||
330.5 MPa Show Material materials with Límite elástico of 330.5 MPa | Predicted Value, RP1 Transverse | |||||
489.3 MPa Show Material materials with Límite elástico of 489.3 MPa | Predicted Value, RP02 Transverse | |||||
539.7 MPa Show Material materials with Límite elástico of 539.7 MPa | Predicted Value, RP05 | |||||
541.5 MPa Show Material materials with Límite elástico of 541.5 MPa | Predicted Value, Transverse | |||||
724.4 MPa Show Material materials with Límite elástico of 724.4 MPa | Predicted Value, RP002 | |||||
20 °C | 630 MPa Show Material materials with Límite elástico of 630 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
20 °C | 670 MPa Show Material materials with Límite elástico of 670 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
20 °C | 690 MPa Show Material materials with Límite elástico of 690 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
50 °C | 610 MPa Show Material materials with Límite elástico of 610 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
50 °C | 650 MPa Show Material materials with Límite elástico of 650 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
50 °C | 670 MPa Show Material materials with Límite elástico of 670 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
100 °C | 585 MPa Show Material materials with Límite elástico of 585 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
100 °C | 625 MPa Show Material materials with Límite elástico of 625 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
100 °C | 645 MPa Show Material materials with Límite elástico of 645 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
150 °C | 555 MPa Show Material materials with Límite elástico of 555 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
150 °C | 595 MPa Show Material materials with Límite elástico of 595 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
150 °C | 615 MPa Show Material materials with Límite elástico of 615 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
200 °C | 535 MPa Show Material materials with Límite elástico of 535 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
200 °C | 575 MPa Show Material materials with Límite elástico of 575 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
200 °C | 595 MPa Show Material materials with Límite elástico of 595 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
250 °C | 515 MPa Show Material materials with Límite elástico of 515 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
250 °C | 555 MPa Show Material materials with Límite elástico of 555 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
250 °C | 575 MPa Show Material materials with Límite elástico of 575 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
300 °C | 510 MPa Show Material materials with Límite elástico of 510 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
300 °C | 550 MPa Show Material materials with Límite elástico of 550 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
300 °C | 570 MPa Show Material materials with Límite elástico of 570 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
Módulo de cizallamiento | 79.6 GPa Show Material materials with Módulo de cizallamiento of 79.6 GPa | Predicted Value | ||||
Módulo elástico | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel | ||||
Resistencia a la tracción | 20 °C | 720 - 940 MPa Show Material materials with Resistencia a la tracción of 720 - 940 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | |
20 °C | 720 - 900 MPa Show Material materials with Resistencia a la tracción of 720 - 900 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
20 °C | 770 - 940 MPa Show Material materials with Resistencia a la tracción of 770 - 940 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
20 °C | 770 - 900 MPa Show Material materials with Resistencia a la tracción of 770 - 900 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
Resistencia al cizallamiento | 598.9 MPa Show Material materials with Resistencia al cizallamiento of 598.9 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 441.4 J/(kg·K) Show Material materials with Calor específico of 441.4 J/(kg·K) | Predicted Value |
Coeficiente de dilatación térmica | 12.01 1/K Show Material materials with Coeficiente de dilatación térmica of 12.01 1/K | Predicted Value |
Conductividad térmica | 34.55 W/(m·K) Show Material materials with Conductividad térmica of 34.55 W/(m·K) | Predicted Value |
Eléctrico
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
0.015 % Show Material materials with Azufre of 0.015 % | quenched and tempered (+QT) | EN 10028-6 | Flat | |
Boro | 0.005 % Show Material materials with Boro of 0.005 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Carbono | 0.2 % Show Material materials with Carbono of 0.2 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Circonio | 0.15 % Show Material materials with Circonio of 0.15 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Cobre | 0.3 % Show Material materials with Cobre of 0.3 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Cromo | 1.5 % Show Material materials with Cromo of 1.5 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Fósforo | 0.025 % Show Material materials with Fósforo of 0.025 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Manganeso | 1.7 % Show Material materials with Manganeso of 1.7 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Molibdeno | 0.7 % Show Material materials with Molibdeno of 0.7 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Niobio | 0.06 % Show Material materials with Niobio of 0.06 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Nitrógeno | 0.015 % Show Material materials with Nitrógeno of 0.015 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Níquel | 2.5 % Show Material materials with Níquel of 2.5 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Silicona | 0.8 % Show Material materials with Silicona of 0.8 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Titanio | 0.05 % Show Material materials with Titanio of 0.05 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Vanadio | 0.12 % Show Material materials with Vanadio of 0.12 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |