Unclassified Low Alloy Steel
EN 10025-6 Grade S620QL1 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10025-6 Grade S690QL1 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-6 Grade P690QH quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TM00Acero bajo en carbono
EN 10277-2 Grade St52-3 cold drawnAcero bajo en carbono
EN 10277-2 Grade ZSt52-3 cold drawnAcero bajo en carbono
EN 10277-2 Grade St 50-2 cold drawnAcero bajo en carbono
EN 10277-2 Grade St 60-2 cold drawnAcero bajo en carbono
EN 10277-2 Grade St 70-2 cold drawnAcero de alto carbono
EN 10083-2 Grade C60E quenched and tempered (+QT)Acero de alto carbono
EN 10083-2 Grade C60E quenched and tempered (+QT)