Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.9 g/cm³ Show Material materials with Densidad of 7.9 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Austenitic Stainless Steel |
Dureza Brinell | 20.0 °C | 215 [-] Show Material materials with Dureza Brinell of 215 [-] | |
Elongación | 20.0 °C | 15 - 35 % Show Material materials with Elongación of 15 - 35 % | |
Límite elástico Rp 0,2 | 20.0 °C | 185 - 400 MPa Show Material materials with Límite elástico Rp 0,2 of 185 - 400 MPa | |
Límite elástico Rp 1,0 | 20.0 °C | 220 MPa Show Material materials with Límite elástico Rp 1,0 of 220 MPa | |
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Austenitic Stainless Steel |
Módulo elástico | 20.0 °C | 200 GPa Show Material materials with Módulo elástico of 200 GPa | |
100.0 °C | 194 GPa Show Material materials with Módulo elástico of 194 GPa | ||
200.0 °C | 186 GPa Show Material materials with Módulo elástico of 186 GPa | ||
300.0 °C | 179 GPa Show Material materials with Módulo elástico of 179 GPa | ||
400.0 °C | 172 GPa Show Material materials with Módulo elástico of 172 GPa | ||
500.0 °C | 165 GPa Show Material materials with Módulo elástico of 165 GPa | ||
Resistencia a la tracción | 20.0 °C | 500 - 1100 MPa Show Material materials with Resistencia a la tracción of 500 - 1100 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 440 J/(kg·K) Show Material materials with Calor específico of 440 J/(kg·K) | Typical for Austenitic Stainless Steel |
Coeficiente de dilatación térmica | 23.0 °C | 1.7E-5 - 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 - 1.9E-5 1/K | Typical for Austenitic Stainless Steel |
Conductividad térmica | 23.0 °C | 11 - 21 W/(m·K) Show Material materials with Conductividad térmica of 11 - 21 W/(m·K) | Typical for Austenitic Stainless Steel |
Temperatura de fusión | 1230 - 1480 °C Show Material materials with Temperatura de fusión of 1230 - 1480 °C | Typical for Austenitic Stainless Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 8.5E-7 Ω·m Show Material materials with Resistividad eléctrica of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.15 - 0.35 % Show Material materials with Azufre of 0.15 - 0.35 % |
Carbono | 0.08 % Show Material materials with Carbono of 0.08 % |
Cobre | 1.4 - 1.8 % Show Material materials with Cobre of 1.4 - 1.8 % |
Cromo | 17 - 19 % Show Material materials with Cromo of 17 - 19 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Manganeso | 2 % Show Material materials with Manganeso of 2 % |
Molibdeno | 0.6 % Show Material materials with Molibdeno of 0.6 % |
Nitrógeno | 0.11 % Show Material materials with Nitrógeno of 0.11 % |
Níquel | 8 - 10 % Show Material materials with Níquel of 8 - 10 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |