General
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 1000 Series Aluminium | ||||
Dureza Brinell | 18.0 [-] Show Material materials with Dureza Brinell of 18.0 [-] | F | EN 573-3, EN 485 | |||
19.0 [-] Show Material materials with Dureza Brinell of 19.0 [-] | F | EN 573-3, EN 570 | ||||
20.0 °C | 18.0 [-] Show Material materials with Dureza Brinell of 18.0 [-] | F | DIN 1712-3, EN 573-3, EN 573-4 | Profile, Rod, Tube | ||
Elongación | 20.0 °C | 22.0 % Show Material materials with Elongación of 22.0 % | F | DIN 1712-3, EN 573-3, EN 573-4 | Profile, Rod, Tube | A10 |
20.0 °C | 25.0 % Show Material materials with Elongación of 25.0 % | F | DIN 1712-3, EN 573-3, EN 573-4 | Profile, Rod, Tube | ||
Módulo de cizallamiento | 20.0 °C | 25.0 GPa Show Material materials with Módulo de cizallamiento of 25.0 GPa | F | DIN 1712-3, EN 573-3, EN 573-4 | Profile, Rod, Tube | |
Módulo elástico | 70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | F | EN 573-3, EN 1715-3, EN 1715-4, EN 485, EN 570 | |||
20.0 °C | 60.0 - 70.0 GPa Show Material materials with Módulo elástico of 60.0 - 70.0 GPa | F | DIN 1712-3, EN 573-3, EN 573-4 | Profile, Rod, Tube | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 1000 Series Aluminium | ||||
Resistencia a la tracción | 60.0 MPa Show Material materials with Resistencia a la tracción of 60.0 MPa | F | EN 573-3, EN 485 | |||
80.0 - 110.0 MPa Show Material materials with Resistencia a la tracción of 80.0 - 110.0 MPa | F | EN 573-3, EN 1715-3, EN 1715-4 | ||||
20.0 °C | 55.0 MPa Show Material materials with Resistencia a la tracción of 55.0 MPa | F | DIN 1712-3, EN 573-3, EN 573-4 | Profile | ||
20.0 °C | 60.0 MPa Show Material materials with Resistencia a la tracción of 60.0 MPa | F | DIN 1712-3, EN 573-3, EN 573-4 | Rod, Tube |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Calor específico | 20.0 °C | 921.0 J/(kg·K) Show Material materials with Calor específico of 921.0 J/(kg·K) | F | DIN 1712-3, EN 573-3, EN 573-4 | Profile, Rod, Tube |
Coeficiente de dilatación térmica | 20 °C | 2.35e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.35e-05 1/K | F | EN 573-3, EN 1715-3, EN 1715-4, EN 485, EN 570 | |
100 °C | 2.35e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.35e-05 1/K | F | EN 573-3, EN 1715-3, EN 1715-4, EN 485, EN 570 | ||
Conductividad térmica | 225 W/(m·K) Show Material materials with Conductividad térmica of 225 W/(m·K) | F | EN 573-3, EN 1715-3, EN 1715-4, EN 485, EN 570 | ||
20.0 °C | 215.0 W/(m·K) Show Material materials with Conductividad térmica of 215.0 W/(m·K) | F | DIN 1712-3, EN 573-3, EN 573-4 | Profile, Rod, Tube | |
Temperatura de fusión | 659.0 °C Show Material materials with Temperatura de fusión of 659.0 °C | F | EN 573-3, EN 1715-3, EN 1715-4, EN 485, EN 570 |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Conductividad eléctrica | 34500000.0 - 35000000.0 S/m Show Material materials with Conductividad eléctrica of 34500000.0 - 35000000.0 S/m | F | EN 573-3, EN 1715-3, EN 1715-4, EN 485, EN 570 | ||
20.0 °C | 36400000.0 - 37000000.0 S/m Show Material materials with Conductividad eléctrica of 36400000.0 - 37000000.0 S/m | F | DIN 1712-3, EN 573-3, EN 573-4 | Profile, Rod, Tube | |
Resistividad eléctrica | 2.86e-08 - 2.9e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.86e-08 - 2.9e-08 Ω·m | F | EN 573-3, EN 1715-3, EN 1715-4, EN 485, EN 570 |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 99.8 % Show Material materials with Aluminio of 99.8 % | F | EN 573-3, EN 1715-3, EN 1715-4, EN 485, EN 570 | |
Cobre | 0.03 % Show Material materials with Cobre of 0.03 % | F | DIN 1712-3, EN 573-3, EN 573-4, EN 1715-3, EN 1715-4, EN 485, EN 570 | Profile, Rod, Tube |
Galio | 0.03 % Show Material materials with Galio of 0.03 % | F | DIN 1712-3, EN 573-3, EN 573-4, EN 1715-3, EN 1715-4, EN 485, EN 570 | Profile, Rod, Tube |
Hierro | 0.15 % Show Material materials with Hierro of 0.15 % | F | DIN 1712-3, EN 573-3, EN 573-4 | Profile, Rod, Tube |
0.15 % Show Material materials with Hierro of 0.15 % | F | EN 573-3, EN 1715-3, EN 1715-4, EN 485, EN 570 | ||
Magnesio | 0.02 % Show Material materials with Magnesio of 0.02 % | F | DIN 1712-3, EN 573-3, EN 573-4, EN 1715-3, EN 1715-4, EN 485, EN 570 | Profile, Rod, Tube |
Manganeso | 0.02 % Show Material materials with Manganeso of 0.02 % | F | DIN 1712-3, EN 573-3, EN 573-4, EN 1715-3, EN 1715-4, EN 485, EN 570 | Profile, Rod, Tube |
Silicona | 0.15 % Show Material materials with Silicona of 0.15 % | F | DIN 1712-3, EN 573-3, EN 573-4, EN 1715-3, EN 1715-4, EN 485, EN 570 | Profile, Rod, Tube |
Titanio | 0.02 % Show Material materials with Titanio of 0.02 % | F | DIN 1712-3, EN 573-3, EN 573-4, EN 1715-3, EN 1715-4, EN 485, EN 570 | Profile, Rod, Tube |
Zinc | 0.06 % Show Material materials with Zinc of 0.06 % | F | DIN 1712-3, EN 573-3, EN 573-4, EN 1715-3, EN 1715-4, EN 485, EN 570 | Profile, Rod, Tube |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: very good, Protective: very good | |
Brazing | hard brazing (with flux/ without flux): very good / very good, friction soldering: very good, soft brazing with flux: very good | |
Workability | Bending / Spinning (cold): very good / very good, Impact extrusion (cold): very good, Deep drawing / upsetting (Condition) very good (H14) / very good (H12) |