General
Property | Temperature | Value | Related Standards |
---|---|---|---|
Densidad | 20.0 °C | 2.69 g/cm³ Show Material materials with Densidad of 2.69 g/cm³ | DIN 1725-1, EN 573-3, EN 573-4 |
Mecánica
Property | Temperature | Value | Related Standards | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 6000 Series Aluminium | ||
Módulo de cizallamiento | 20.0 °C | 26.5 - 27.0 GPa Show Material materials with Módulo de cizallamiento of 26.5 - 27.0 GPa | DIN 1725-1, EN 573-3, EN 573-4 | |
Módulo elástico | 20.0 °C | 68.0 GPa Show Material materials with Módulo elástico of 68.0 GPa | DIN 1725-1, EN 573-3, EN 573-4 | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 6000 Series Aluminium |
Aplicaciones térmicas
Property | Temperature | Value | Related Standards | Comment |
---|---|---|---|---|
Calor específico | 887.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 887.0 - 963.0 J/(kg·K) | Typical for Wrought 6000 Series Aluminium | ||
Coeficiente de dilatación térmica | 1.6e-05 - 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6e-05 - 2.4e-05 1/K | Typical for Wrought 6000 Series Aluminium | ||
Conductividad térmica | 20.0 °C | 210.0 W/(m·K) Show Material materials with Conductividad térmica of 210.0 W/(m·K) | DIN 1725-1, EN 573-3, EN 573-4 | |
Temperatura de fusión | 555.0 - 655.0 °C Show Material materials with Temperatura de fusión of 555.0 - 655.0 °C | Typical for Wrought 6000 Series Aluminium |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 21000000.0 - 34000000.0 S/m Show Material materials with Conductividad eléctrica of 21000000.0 - 34000000.0 S/m | Typical for Wrought 6000 Series Aluminium |
Resistividad eléctrica | 2.9e-08 - 5e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.9e-08 - 5e-08 Ω·m | Typical for Wrought 6000 Series Aluminium |
Chemical properties
Property | Value | Related Standards |
---|---|---|
Cobre | 0.02 Show Material materials with Cobre of 0.02 | DIN 1725-1, EN 573-3, EN 573-4 |
Hierro | 0.1 - 0.3 % Show Material materials with Hierro of 0.1 - 0.3 % | DIN 1725-1, EN 573-3, EN 573-4 |
Magnesio | 0.35 - 0.6 % Show Material materials with Magnesio of 0.35 - 0.6 % | DIN 1725-1, EN 573-3, EN 573-4 |
Silicona | 0.5 - 0.6 % Show Material materials with Silicona of 0.5 - 0.6 % | DIN 1725-1, EN 573-3, EN 573-4 |
Zinc | 0.15 Show Material materials with Zinc of 0.15 | DIN 1725-1, EN 573-3, EN 573-4 |
Technological properties
Property | ||
---|---|---|
Workability | Excellent workability. |