General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Densidad | 20.0 °C | 2.64 g/cm³ Show Material materials with Densidad of 2.64 g/cm³ | H32 | WL 3.3354, DIN 1725-1 | Wire |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 5000 Series Aluminium | ||||
Módulo de cizallamiento | 26.0 - 26.5 GPa Show Material materials with Módulo de cizallamiento of 26.0 - 26.5 GPa | Typical for Wrought 5000 Series Aluminium | ||||
Módulo elástico | 20.0 °C | 71.0 GPa Show Material materials with Módulo elástico of 71.0 GPa | H32 | WL 3.3354, DIN 1725-1 | Wire | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | ||||
Resistencia a la tracción | 20.0 °C | 300.0 - 360.0 MPa Show Material materials with Resistencia a la tracción of 300.0 - 360.0 MPa | H32 | WL 3.3354, DIN 1725-1 | Wire | |
Resistencia al cizallamiento | 20.0 °C | 170.0 MPa Show Material materials with Resistencia al cizallamiento of 170.0 MPa | H32 | WL 3.3354, DIN 1725-1 | Wire | Transverse |
20.0 °C | 170.0 - 193.0 MPa Show Material materials with Resistencia al cizallamiento of 170.0 - 193.0 MPa | H32 | WL 3.3354, DIN 1725-1 | Transverse | ||
20.0 °C | 170.0 MPa Show Material materials with Resistencia al cizallamiento of 170.0 MPa | H32 | WL 3.3354, DIN 1725-1 | Wire | ||
20.0 °C | 193.0 MPa Show Material materials with Resistencia al cizallamiento of 193.0 MPa | H32 | WL 3.3354, DIN 1725-1 | Transverse |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 20.0 °C | 904.0 J/(kg·K) Show Material materials with Calor específico of 904.0 J/(kg·K) | H32 | WL 3.3354, DIN 1725-1 | Wire | |
Coeficiente de dilatación térmica | 2.2e-05 - 2.5e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.2e-05 - 2.5e-05 1/K | Typical for Wrought 5000 Series Aluminium | ||||
Conductividad térmica | 20.0 °C | 110.0 - 140.0 W/(m·K) Show Material materials with Conductividad térmica of 110.0 - 140.0 W/(m·K) | H32 | WL 3.3354, DIN 1725-1 | Wire | |
Temperatura de fusión | 560.0 - 655.0 °C Show Material materials with Temperatura de fusión of 560.0 - 655.0 °C | Typical for Wrought 5000 Series Aluminium | ||||
Temperatura máx. de funcionamiento | 150.0 °C Show Material materials with Temperatura máx. de funcionamiento of 150.0 °C | Typical for Wrought 5000 Series Aluminium |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Conductividad eléctrica | 20.0 °C | 15000000.0 - 19000000.0 S/m Show Material materials with Conductividad eléctrica of 15000000.0 - 19000000.0 S/m | H32 | WL 3.3354, DIN 1725-1 | Wire | |
Resistividad eléctrica | 3.3e-08 - 5e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.3e-08 - 5e-08 Ω·m | Typical for Wrought 5000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.1 Show Material materials with Cobre of 0.1 | H32 | WL 3.3354, DIN 1725-1 | Wire |
Cromo | 0.2 Show Material materials with Cromo of 0.2 | H32 | WL 3.3354, DIN 1725-1 | Wire |
Hierro | 0.5 Show Material materials with Hierro of 0.5 | H32 | WL 3.3354, DIN 1725-1 | Wire |
Magnesio | 4.5 - 5.6 % Show Material materials with Magnesio of 4.5 - 5.6 % | H32 | WL 3.3354, DIN 1725-1 | Wire |
Manganeso | 0.1 - 0.6 % Show Material materials with Manganeso of 0.1 - 0.6 % | H32 | WL 3.3354, DIN 1725-1 | Wire |
Silicona | 0.4 Show Material materials with Silicona of 0.4 | H32 | WL 3.3354, DIN 1725-1 | Wire |
Zinc | 0.2 Show Material materials with Zinc of 0.2 | H32 | WL 3.3354, DIN 1725-1 | Wire |
Technological properties
Property | ||
---|---|---|
Workability | Good workability. |