General
Property | Value | Comment |
---|---|---|
Densidad | 2.65 - 2.7 g/cm³ Show Material materials with Densidad of 2.65 - 2.7 g/cm³ | Typical for Cast 3xx.x Series Aluminium |
Mecánica
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium | ||
Elongación | 2.0 - 4.0 % Show Material materials with Elongación of 2.0 - 4.0 % | T6 | DIN 1725-2 | |
Módulo de cizallamiento | 2.8 GPa Show Material materials with Módulo de cizallamiento of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium | ||
Módulo elástico | 73.0 - 80.0 GPa Show Material materials with Módulo elástico of 73.0 - 80.0 GPa | Typical for Cast 3xx.x Series Aluminium |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 960.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 960.0 - 963.0 J/(kg·K) | Typical for Cast 3xx.x Series Aluminium |
Coeficiente de dilatación térmica | 1.6e-05 - 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6e-05 - 2.3e-05 1/K | Typical for Cast 3xx.x Series Aluminium |
Conductividad térmica | 130.0 - 180.0 W/(m·K) Show Material materials with Conductividad térmica of 130.0 - 180.0 W/(m·K) | Typical for Cast 3xx.x Series Aluminium |
Temperatura de fusión | 505.0 - 770.0 °C Show Material materials with Temperatura de fusión of 505.0 - 770.0 °C | Typical for Cast 3xx.x Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Cobre | 0.05 Show Material materials with Cobre of 0.05 | T6 | DIN 1725-2 |
Hierro | 0.19 Show Material materials with Hierro of 0.19 | T6 | DIN 1725-2 |
Magnesio | 0.25 - 0.45 % Show Material materials with Magnesio of 0.25 - 0.45 % | T6 | DIN 1725-2 |
Manganeso | 0.1 Show Material materials with Manganeso of 0.1 | T6 | DIN 1725-2 |
Silicona | 6.5 - 7.5 % Show Material materials with Silicona of 6.5 - 7.5 % | T6 | DIN 1725-2 |
Titanio | 0.08 - 0.25 % Show Material materials with Titanio of 0.08 - 0.25 % | T6 | DIN 1725-2 |
Zinc | 0.07 Show Material materials with Zinc of 0.07 | T6 | DIN 1725-2 |
Technological properties
Property | ||
---|---|---|
Anodizing | not recommended | |
Corrosion properties | Good against water (class B) and see water (class X) |