General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Densidad | 20.0 °C | 2.7 g/cm³ Show Material materials with Densidad of 2.7 g/cm³ | T3 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3214-1 | Sheet, Flat |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 6000 Series Aluminium | ||||
Dureza Brinell | 20.0 °C | 60.0 [-] Show Material materials with Dureza Brinell of 60.0 [-] | T3 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3214-1 | Sheet, Flat | |
Elongación | 20.0 °C | 10.0 % Show Material materials with Elongación of 10.0 % | T3 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3214-1 | Sheet | A10 |
20.0 °C | 12.0 % Show Material materials with Elongación of 12.0 % | T3 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3214-1 | Flat | A10 | |
20.0 °C | 12.0 % Show Material materials with Elongación of 12.0 % | T3 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3214-1 | Sheet | ||
20.0 °C | 14.0 % Show Material materials with Elongación of 14.0 % | T3 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3214-1 | Flat | ||
Módulo de cizallamiento | 20.0 °C | 26.2 Show Material materials with Módulo de cizallamiento of 26.2 | T3 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3214-1 | Sheet, Flat | |
Módulo elástico | 20.0 °C | 68.3 - 69.6 GPa Show Material materials with Módulo elástico of 68.3 - 69.6 GPa | T3 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3214-1 | Sheet, Flat | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 6000 Series Aluminium | ||||
Resistencia a la tracción | 20.0 °C | 205.0 MPa Show Material materials with Resistencia a la tracción of 205.0 MPa | T3 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3214-1 | Sheet, Flat |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 20.0 °C | 870.0 J/(kg·K) Show Material materials with Calor específico of 870.0 J/(kg·K) | T3 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3214-1 | Sheet, Flat | |
Coeficiente de dilatación térmica | 1.6e-05 - 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6e-05 - 2.4e-05 1/K | Typical for Wrought 6000 Series Aluminium | ||||
Conductividad térmica | 20.0 °C | 150.0 - 165.0 W/(m·K) Show Material materials with Conductividad térmica of 150.0 - 165.0 W/(m·K) | T3 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3214-1 | Sheet, Flat | |
Temperatura de fusión | 555.0 - 655.0 °C Show Material materials with Temperatura de fusión of 555.0 - 655.0 °C | Typical for Wrought 6000 Series Aluminium |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Conductividad eléctrica | 20.0 °C | 20000000.0 - 30000000.0 S/m Show Material materials with Conductividad eléctrica of 20000000.0 - 30000000.0 S/m | T3 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3214-1 | Sheet, Flat | |
Resistividad eléctrica | 2.9e-08 - 5e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.9e-08 - 5e-08 Ω·m | Typical for Wrought 6000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.15 - 0.4 % Show Material materials with Cobre of 0.15 - 0.4 % | T3 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3214-1 | Sheet, Flat |
Cromo | 0.04 - 0.35 % Show Material materials with Cromo of 0.04 - 0.35 % | T3 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3214-1 | Sheet, Flat |
Hierro | 0.7 Show Material materials with Hierro of 0.7 | T3 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3214-1 | Sheet, Flat |
Magnesio | 0.8 - 1.2 % Show Material materials with Magnesio of 0.8 - 1.2 % | T3 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3214-1 | Sheet, Flat |
Manganeso | 0.15 Show Material materials with Manganeso of 0.15 | T3 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3214-1 | Sheet, Flat |
Silicona | 0.4 - 0.8 % Show Material materials with Silicona of 0.4 - 0.8 % | T3 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3214-1 | Sheet, Flat |
Titanio | 0.15 Show Material materials with Titanio of 0.15 | T3 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3214-1 | Sheet, Flat |
Zinc | 0.25 Show Material materials with Zinc of 0.25 | T3 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3214-1 | Sheet, Flat |
Technological properties
Property | ||
---|---|---|
Workability | Excellent workability. |