Chemical properties
Property | Value | Related Standards |
---|---|---|
Berilio | 4.5 - 6.0 % Show Material materials with Berilio of 4.5 - 6.0 % | EN 575, DIN 1725-3 |
Boro | 0.01 % Show Material materials with Boro of 0.01 % | EN 575, DIN 1725-3 |
Estaño | 0.02 % Show Material materials with Estaño of 0.02 % | EN 575, DIN 1725-3 |
Hierro | 0.3 % Show Material materials with Hierro of 0.3 % | EN 575, DIN 1725-3 |
0.30 % Show Material materials with Hierro of 0.30 % | EN 575 | |
Magnesio | 0.5 % Show Material materials with Magnesio of 0.5 % | EN 575, DIN 1725-3 |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % | EN 575, DIN 1725-3 |
Silicona | 0.3 % Show Material materials with Silicona of 0.3 % | EN 575, DIN 1725-3 |
Zinc | 0.04 % Show Material materials with Zinc of 0.04 % | EN 575, DIN 1725-3 |