Chemical properties
Property | Value | Related Standards |
---|---|---|
Cobre | 0.2 % Show Material materials with Cobre of 0.2 % | EN 575, DIN 1725-3 |
Cromo | 0.1 % Show Material materials with Cromo of 0.1 % | EN 575, DIN 1725-3 |
Hierro | 0.7 % Show Material materials with Hierro of 0.7 % | EN 575, DIN 1725-3 |
0.70 % Show Material materials with Hierro of 0.70 % | EN 575 | |
Magnesio | 0.5 % Show Material materials with Magnesio of 0.5 % | EN 575, DIN 1725-3 |
Manganeso | 0.4 % Show Material materials with Manganeso of 0.4 % | EN 575, DIN 1725-3 |
Níquel | 0.2 % Show Material materials with Níquel of 0.2 % | EN 575, DIN 1725-3 |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % | EN 575, DIN 1725-3 |
Titanio | 4.5 - 5.5 % Show Material materials with Titanio of 4.5 - 5.5 % | EN 575, DIN 1725-3 |
Vanadio | 0.3 % Show Material materials with Vanadio of 0.3 % | EN 575, DIN 1725-3 |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % | EN 575, DIN 1725-3 |