General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 2.65 - 2.7 g/cm³ Show Material materials with Densidad of 2.65 - 2.7 g/cm³ | Typical for Cast 3xx.x Series Aluminium |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium |
Módulo de cizallamiento | 23.0 °C | 2.8 GPa Show Material materials with Módulo de cizallamiento of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium |
Módulo elástico | 23.0 °C | 73 - 80 GPa Show Material materials with Módulo elástico of 73 - 80 GPa | Typical for Cast 3xx.x Series Aluminium |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 960 - 963 J/(kg·K) Show Material materials with Calor específico of 960 - 963 J/(kg·K) | Typical for Cast 3xx.x Series Aluminium |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 - 2.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 2.3E-5 1/K | Typical for Cast 3xx.x Series Aluminium |
Conductividad térmica | 23.0 °C | 130 - 180 W/(m·K) Show Material materials with Conductividad térmica of 130 - 180 W/(m·K) | Typical for Cast 3xx.x Series Aluminium |
Temperatura de fusión | 505 - 770 °C Show Material materials with Temperatura de fusión of 505 - 770 °C | Typical for Cast 3xx.x Series Aluminium |
Chemical properties
Property | Value |
---|---|
Aluminio | 80.9999 - 88.8999 % Show Material materials with Aluminio of 80.9999 - 88.8999 % |
Cobre | 1.5 - 3.5 % Show Material materials with Cobre of 1.5 - 3.5 % |
Estaño | 0.3 % Show Material materials with Estaño of 0.3 % |
Hierro | 0.9 % Show Material materials with Hierro of 0.9 % |
Magnesio | 0.3 % Show Material materials with Magnesio of 0.3 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Níquel | 0.5 % Show Material materials with Níquel of 0.5 % |
Silicona | 9.6 - 12 % Show Material materials with Silicona of 9.6 - 12 % |
Zinc | 1 % Show Material materials with Zinc of 1 % |