General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 2.7 g/cm³ Show Material materials with Densidad of 2.7 g/cm³ | Typical for Wrought 1000 Series Aluminium |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 1000 Series Aluminium |
Módulo de cizallamiento | 23.0 °C | 25.9 GPa Show Material materials with Módulo de cizallamiento of 25.9 GPa | Typical for Wrought 1000 Series Aluminium |
Módulo elástico | 23.0 °C | 68 - 70 GPa Show Material materials with Módulo elástico of 68 - 70 GPa | Typical for Wrought 1000 Series Aluminium |
Plane-Strain Fracture Toughnes | 23.0 °C | 22 - 35 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22 - 35 MPa·√m | Typical for Wrought 1000 Series Aluminium |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 900 - 963 J/(kg·K) Show Material materials with Calor específico of 900 - 963 J/(kg·K) | Typical for Wrought 1000 Series Aluminium |
Coeficiente de dilatación térmica | 23.0 °C | 2.2E-5 - 2.5E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.2E-5 - 2.5E-5 1/K | Typical for Wrought 1000 Series Aluminium |
Conductividad térmica | 23.0 °C | 167 - 244 W/(m·K) Show Material materials with Conductividad térmica of 167 - 244 W/(m·K) | Typical for Wrought 1000 Series Aluminium |
Temperatura de fusión | 645 - 660 °C Show Material materials with Temperatura de fusión of 645 - 660 °C | Typical for Wrought 1000 Series Aluminium |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Conductividad eléctrica | 23.0 °C | 3.30E+7 - 3.80E+7 S/m Show Material materials with Conductividad eléctrica of 3.30E+7 - 3.80E+7 S/m | Typical for Wrought 1000 Series Aluminium |
Resistividad eléctrica | 23.0 °C | 2.7E-8 - 3E-8 Ω·m Show Material materials with Resistividad eléctrica of 2.7E-8 - 3E-8 Ω·m | Typical for Wrought 1000 Series Aluminium |
Chemical properties
Property | Value |
---|---|
Aluminio | 98.4699 - 99.7999 % Show Material materials with Aluminio of 98.4699 - 99.7999 % |
Cobre | 0.2 % Show Material materials with Cobre of 0.2 % |
Hierro | 0.25 % Show Material materials with Hierro of 0.25 % |
Magnesio | 0.2 - 0.6 % Show Material materials with Magnesio of 0.2 - 0.6 % |
Manganeso | 0.2 % Show Material materials with Manganeso of 0.2 % |
Silicona | 0.15 % Show Material materials with Silicona of 0.15 % |
Zinc | 0.03 % Show Material materials with Zinc of 0.03 % |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent | |
Workability | Excellent workability. |