General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Chromium Molybdenum Steel |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Chromium Molybdenum Steel | |||
Elongación | 15.2 % Show Material materials with Elongación of 15.2 % | Predicted Value, Transverse | |||
16.6 % Show Material materials with Elongación of 16.6 % | Predicted Value, A200 | ||||
18.1 % Show Material materials with Elongación of 18.1 % | Predicted Value, A80 | ||||
18.4 % Show Material materials with Elongación of 18.4 % | Predicted Value, A5 | ||||
19.0 % Show Material materials with Elongación of 19.0 % | Predicted Value, A80 Transverse | ||||
20.1 % Show Material materials with Elongación of 20.1 % | Predicted Value, A50 | ||||
20.7 % Show Material materials with Elongación of 20.7 % | Predicted Value | ||||
Estricción | 41.7 % Show Material materials with Estricción of 41.7 % | Predicted Value, Transverse | |||
42.9 % Show Material materials with Estricción of 42.9 % | Predicted Value | ||||
Módulo de cizallamiento | 79.6 GPa Show Material materials with Módulo de cizallamiento of 79.6 GPa | Predicted Value | |||
Módulo elástico | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Chromium Molybdenum Steel | |||
Resistencia a la tracción | 480 MPa Show Material materials with Resistencia a la tracción of 480 MPa | As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPa | ASTM A829 | Plate | |
Resistencia al cizallamiento | 514.4 MPa Show Material materials with Resistencia al cizallamiento of 514.4 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 448 - 502 J/(kg·K) Show Material materials with Calor específico of 448 - 502 J/(kg·K) | Typical for Chromium Molybdenum Steel |
Coeficiente de dilatación térmica | 1.1e-05 - 1.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.1e-05 - 1.4e-05 1/K | Typical for Chromium Molybdenum Steel |
Conductividad térmica | 36 - 43 W/(m·K) Show Material materials with Conductividad térmica of 36 - 43 W/(m·K) | Typical for Chromium Molybdenum Steel |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel |
Eléctrico
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Azufre | 0.04 % Show Material materials with Azufre of 0.04 % | As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPa | ASTM A829 | Plate |
Carbono | 0.36 - 0.44 % Show Material materials with Carbono of 0.36 - 0.44 % | As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPa | ASTM A829 | Plate |
Cromo | 0.8 - 1.1 % Show Material materials with Cromo of 0.8 - 1.1 % | As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPa | ASTM A829 | Plate |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % | As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPa | ASTM A829 | Plate |
Manganeso | 0.75 - 1 % Show Material materials with Manganeso of 0.75 - 1 % | As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPa | ASTM A829 | Plate |
Molibdeno | 0.15 - 0.25 % Show Material materials with Molibdeno of 0.15 - 0.25 % | As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPa | ASTM A829 | Plate |
Silicona | 0.15 - 0.35 % Show Material materials with Silicona of 0.15 - 0.35 % | As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPa | ASTM A829 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |