General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Densidad | 2.75 g/cm³ Show Material materials with Densidad of 2.75 g/cm³ | H13 | EN 573-3, EN 1301 | Wire | |
20.0 °C | 2.74 g/cm³ Show Material materials with Densidad of 2.74 g/cm³ | H13 | EN 573-3 | Wire |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 2000 Series Aluminium | ||||
Elongación | 5.0 % Show Material materials with Elongación of 5.0 % | H13 | EN 573-3, EN 1301 | Wire | ||
20.0 °C | 20.0 % Show Material materials with Elongación of 20.0 % | H13 | EN 573-3 | Wire | A100 | |
Módulo de cizallamiento | 20.0 °C | 25.5 GPa Show Material materials with Módulo de cizallamiento of 25.5 GPa | H13 | EN 573-3 | Wire | |
Módulo elástico | 70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | H13 | EN 573-3, EN 1301 | Wire | ||
20.0 °C | 67.0 GPa Show Material materials with Módulo elástico of 67.0 GPa | H13 | EN 573-3 | Wire | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 2000 Series Aluminium | ||||
Resistencia a la tracción | 170.0 - 240.0 MPa Show Material materials with Resistencia a la tracción of 170.0 - 240.0 MPa | H13 | EN 573-3, EN 1301 | Wire | ||
20.0 °C | 260.0 MPa Show Material materials with Resistencia a la tracción of 260.0 MPa | H13 | EN 573-3 | Wire |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 20.0 °C | 898.0 J/(kg·K) Show Material materials with Calor específico of 898.0 J/(kg·K) | H13 | EN 573-3 | Wire | |
Coeficiente de dilatación térmica | -50.0 °C | 2.18e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.18e-05 1/K | H13 | EN 573-3 | Wire | |
100.0 °C | 2.34e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.34e-05 1/K | H13 | EN 573-3 | Wire | ||
200.0 °C | 2.45e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.45e-05 1/K | H13 | EN 573-3 | Wire | ||
300.0 °C | 2.56e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.56e-05 1/K | H13 | EN 573-3 | Wire | ||
Conductividad térmica | 20.0 °C | 150.0 - 180.0 W/(m·K) Show Material materials with Conductividad térmica of 150.0 - 180.0 W/(m·K) | H13 | EN 573-3 | Wire | |
Temperatura de fusión | 500.0 - 650.0 °C Show Material materials with Temperatura de fusión of 500.0 - 650.0 °C | Typical for Wrought 2000 Series Aluminium |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Conductividad eléctrica | 20.0 °C | 21000000.0 - 25000000.0 S/m Show Material materials with Conductividad eléctrica of 21000000.0 - 25000000.0 S/m | H13 | EN 573-3 | Wire | |
Resistividad eléctrica | 3.4e-08 - 6e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.4e-08 - 6e-08 Ω·m | Typical for Wrought 2000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 2.2 - 3.0 % Show Material materials with Cobre of 2.2 - 3.0 % | H13 | EN 573-3, EN 1301 | Wire |
Cromo | 0.1 % Show Material materials with Cromo of 0.1 % | H13 | EN 573-3, EN 1301 | Wire |
Hierro | 0.7 % Show Material materials with Hierro of 0.7 % | H13 | EN 573-3 | Wire |
0.70 % Show Material materials with Hierro of 0.70 % | H13 | EN 573-3, EN 1301 | Wire | |
Magnesio | 0.2 - 0.5 % Show Material materials with Magnesio of 0.2 - 0.5 % | H13 | EN 573-3, EN 1301 | Wire |
Manganeso | 0.2 % Show Material materials with Manganeso of 0.2 % | H13 | EN 573-3, EN 1301 | Wire |
Silicona | 0.8 % Show Material materials with Silicona of 0.8 % | H13 | EN 573-3, EN 1301 | Wire |
Zinc | 0.25 % Show Material materials with Zinc of 0.25 % | H13 | EN 573-3, EN 1301 | Wire |
Technological properties
Property | ||
---|---|---|
Brazing | hard brazing (with flux/ without flux): sufficient / sufficient | |
Corrosion properties | Seawater: poor, weathering: poor | |
Workability | Moderate Workability |