General
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Densidad | 20.0 °C | 2.8 g/cm³ Show Material materials with Densidad of 2.8 g/cm³ | F53 | EN 573-3 |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 7000 Series Aluminium | |||
Elongación | -196.0 °C | 9.0 % Show Material materials with Elongación of 9.0 % | F53 | EN 573-3 | |
-80.0 °C | 11.0 % Show Material materials with Elongación of 11.0 % | F53 | EN 573-3 | ||
-28.0 °C | 11.0 % Show Material materials with Elongación of 11.0 % | F53 | EN 573-3 | ||
20.0 °C | 11.0 % Show Material materials with Elongación of 11.0 % | F53 | EN 573-3 | ||
100.0 °C | 14.0 % Show Material materials with Elongación of 14.0 % | F53 | EN 573-3 | ||
150.0 °C | 30.0 % Show Material materials with Elongación of 30.0 % | F53 | EN 573-3 | ||
200.0 °C | 55.0 % Show Material materials with Elongación of 55.0 % | F53 | EN 573-3 | ||
260.0 °C | 65.0 % Show Material materials with Elongación of 65.0 % | F53 | EN 573-3 | ||
315.0 °C | 70.0 % Show Material materials with Elongación of 70.0 % | F53 | EN 573-3 | ||
370.0 °C | 70.0 % Show Material materials with Elongación of 70.0 % | F53 | EN 573-3 | ||
Módulo de cizallamiento | 20.0 °C | 25.0 - 27.0 GPa Show Material materials with Módulo de cizallamiento of 25.0 - 27.0 GPa | F53 | EN 573-3 | |
Módulo elástico | 20.0 °C | 70.0 - 73.0 GPa Show Material materials with Módulo elástico of 70.0 - 73.0 GPa | F53 | EN 573-3 | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 7000 Series Aluminium | |||
Resistencia a la tracción | -196.0 °C | 700.0 MPa Show Material materials with Resistencia a la tracción of 700.0 MPa | F53 | EN 573-3 | |
-80.0 °C | 620.0 MPa Show Material materials with Resistencia a la tracción of 620.0 MPa | F53 | EN 573-3 | ||
-28.0 °C | 590.0 MPa Show Material materials with Resistencia a la tracción of 590.0 MPa | F53 | EN 573-3 | ||
20.0 °C | 570.0 MPa Show Material materials with Resistencia a la tracción of 570.0 MPa | F53 | EN 573-3 | ||
100.0 °C | 485.0 MPa Show Material materials with Resistencia a la tracción of 485.0 MPa | F53 | EN 573-3 | ||
150.0 °C | 215.0 MPa Show Material materials with Resistencia a la tracción of 215.0 MPa | F53 | EN 573-3 | ||
200.0 °C | 110.0 MPa Show Material materials with Resistencia a la tracción of 110.0 MPa | F53 | EN 573-3 | ||
260.0 °C | 75.0 MPa Show Material materials with Resistencia a la tracción of 75.0 MPa | F53 | EN 573-3 | ||
315.0 °C | 55.0 MPa Show Material materials with Resistencia a la tracción of 55.0 MPa | F53 | EN 573-3 | ||
370.0 °C | 40.0 MPa Show Material materials with Resistencia a la tracción of 40.0 MPa | F53 | EN 573-3 |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Calor específico | 20.0 °C | 862.0 J/(kg·K) Show Material materials with Calor específico of 862.0 J/(kg·K) | F53 | EN 573-3 | |
Coeficiente de dilatación térmica | -50.0 °C | 2.16e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.16e-05 1/K | F53 | EN 573-3 | |
100.0 °C | 2.34e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.34e-05 1/K | F53 | EN 573-3 | ||
200.0 °C | 2.43e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.43e-05 1/K | F53 | EN 573-3 | ||
300.0 °C | 2.52e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.52e-05 1/K | F53 | EN 573-3 | ||
Conductividad térmica | 20.0 °C | 130.0 - 160.0 W/(m·K) Show Material materials with Conductividad térmica of 130.0 - 160.0 W/(m·K) | F53 | EN 573-3 | |
Temperatura de fusión | 465.0 - 655.0 °C Show Material materials with Temperatura de fusión of 465.0 - 655.0 °C | Typical for Wrought 7000 Series Aluminium |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Conductividad eléctrica | 20.0 °C | 19000000.0 - 23000000.0 S/m Show Material materials with Conductividad eléctrica of 19000000.0 - 23000000.0 S/m | F53 | EN 573-3 | |
Resistividad eléctrica | 2.9e-08 - 5.6e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.9e-08 - 5.6e-08 Ω·m | Typical for Wrought 7000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Cobre | 1.2 - 2.0 % Show Material materials with Cobre of 1.2 - 2.0 % | F53 | EN 573-3 |
Cromo | 0.18 - 0.28 % Show Material materials with Cromo of 0.18 - 0.28 % | F53 | EN 573-3 |
Hierro | 0.5 Show Material materials with Hierro of 0.5 | F53 | EN 573-3 |
Magnesio | 2.1 - 2.9 % Show Material materials with Magnesio of 2.1 - 2.9 % | F53 | EN 573-3 |
Manganeso | 0.3 Show Material materials with Manganeso of 0.3 | F53 | EN 573-3 |
Silicona | 0.4 Show Material materials with Silicona of 0.4 | F53 | EN 573-3 |
Titanio | 0.2 Show Material materials with Titanio of 0.2 | F53 | EN 573-3 |
Zinc | 5.1 - 6.1 % Show Material materials with Zinc of 5.1 - 6.1 % | F53 | EN 573-3 |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent |