General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mecánica
Property | Value | Comment |
---|---|---|
Coeficiente de Poisson | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Low Carbon Steel |
Módulo de cizallamiento | 82 GPa Show Material materials with Módulo de cizallamiento of 82 GPa | Typical for Low Carbon Steel |
Módulo elástico | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Low Carbon Steel |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 465 J/(kg·K) Show Material materials with Calor específico of 465 J/(kg·K) | Typical for Low Carbon Steel |
Coeficiente de dilatación térmica | 1.32e-05 - 1.38e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.32e-05 - 1.38e-05 1/K | Typical for Low Carbon Steel |
Conductividad térmica | 25 - 93 W/(m·K) Show Material materials with Conductividad térmica of 25 - 93 W/(m·K) | Typical for Low Carbon Steel |
Temperatura de fusión | 1480 - 1526 °C Show Material materials with Temperatura de fusión of 1480 - 1526 °C | Typical for Low Carbon Steel |
Temperatura máx. de funcionamiento | 500 °C Show Material materials with Temperatura máx. de funcionamiento of 500 °C | Typical for Carbon Steel |
Eléctrico
Property | Value | Comment |
---|---|---|
Resistividad eléctrica | 1.43e-07 - 1.74e-07 Ω·m Show Material materials with Resistividad eléctrica of 1.43e-07 - 1.74e-07 Ω·m | Typical for Carbon Steel |
Magnético
Property | Value | Comment |
---|---|---|
Temperatura de Curie | 770 °C Show Material materials with Temperatura de Curie of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminio | 0.02 % Show Material materials with Aluminio of 0.02 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Azufre | 0.035 % Show Material materials with Azufre of 0.035 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Carbono | 0.13 - 0.18 % Show Material materials with Carbono of 0.13 - 0.18 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Cobre | 0.02 % Show Material materials with Cobre of 0.02 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Cromo | 0.02 % Show Material materials with Cromo of 0.02 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Manganeso | 0.3 - 0.6 % Show Material materials with Manganeso of 0.3 - 0.6 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Molibdeno | 0.02 % Show Material materials with Molibdeno of 0.02 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Niobio | 0.08 % Show Material materials with Niobio of 0.08 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Níquel | 0.02 % Show Material materials with Níquel of 0.02 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Silicona | 0.02 % Show Material materials with Silicona of 0.02 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Titanio | 0.08 % Show Material materials with Titanio of 0.08 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Vanadio | 0.08 % Show Material materials with Vanadio of 0.08 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |