OYAK Mining Metallurgy

Claim this profile

About OYAK Mining Metallurgy

we produce hot- and cold-rolled tin-, chrome- and zinc-coated products and plates at international quality standards. Our products provide basic input for sectors such as automotive, white appliances, shipbuilding, pipe manufacture, agricultural instruments, heat industry, electrics-electronics, machinery manufacturing, general construction and packaging, and we lead the development of our country's industry.

Company profile

Headquarters

Ataşehir İstanbul, Turkey

Type

Manufacturer and Processor

Certifications

ISO 14001

Grades provided by the supplier

Grade Shape Equivalent Materials Standard / Norm 

ASTM A615 Grade 40

Wire

ASTM A615 Grade 40

ASTM A615

EN C32D

Bar, Sheet, Coil

EN C32D

ISO 16120-2

EN S235JR

Bar, Sheet, Coil

EN S235JR

EN 10025-2

SAE 1005

Wire

SAE 1005

SAE J403

SAE 1006

Wire

SAE 1006

SAE J403

SAE 1008

Wire

SAE 1008

SAE J403

SAE 1010

Wire

SAE 1010

SAE J403

SAE 1012

Bar, Sheet, Coil

SAE 1012

SAE J403

SAE 1013

Bar, Sheet, Coil

SAE 1013

SAE J403

SAE 1015

Bar, Sheet, Coil

SAE 1015

SAE J403

Showing 1 to 10 of 21 entries

Previous

1
2
3

Next

Locations

Turkey

Turkey

Barbaros Mahallesi Ardıç Sokak No:6

34746 Ataşehir İstanbul

(+90)2165788000

Turkey

Uzunkum No: 7

67330 Karadeniz Ereğli, Zonguldak

(+90)3723232500

Turkey

Gebze Organize Sanayi Bölgesi 700.Sokak No:724

41400 Gebze Kocaeli

(+90)2626792727

Turkey

Manisa Organize Sanayi Bölgesi Hasan Türek Bulvarı No:16

45030 Yunusemre,Manisa

(+90)2362140604

Turkey

Karşı Mahalle Şehit Yüzbaşı Ali Oğuz Bulvarı No: 1

31900 Payas,Hatay

(+90)3267584040

Turkey

Cürek Yolu 5. km

58300 Divriği,Sivas

(+90)3464191121