General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Manganese Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Manganese Steel |
Módulo elástico | 23.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Manganese Steel |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 510 - 553 J/(kg·K) Show Material materials with Calor específico of 510 - 553 J/(kg·K) | Typical for Manganese Steel |
Coeficiente de dilatación térmica | 23.0 °C | 1.33E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.33E-5 1/K | Typical for Manganese Steel |
Conductividad térmica | 23.0 °C | 14 - 16 W/(m·K) Show Material materials with Conductividad térmica of 14 - 16 W/(m·K) | Typical for Manganese Steel |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Manganese Steel |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.02 % Show Material materials with Aluminio of 0.02 % |
Azufre | 0.24 - 0.33 % Show Material materials with Azufre of 0.24 - 0.33 % |
Carbono | 0.4 - 0.48 % Show Material materials with Carbono of 0.4 - 0.48 % |
Cobre | 0.02 % Show Material materials with Cobre of 0.02 % |
Cromo | 0.02 % Show Material materials with Cromo of 0.02 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | balance |
Manganeso | 1.35 - 1.65 % Show Material materials with Manganeso of 1.35 - 1.65 % |
Molibdeno | 0.02 % Show Material materials with Molibdeno of 0.02 % |
Niobio | 0.08 % Show Material materials with Niobio of 0.08 % |
Níquel | 0.02 % Show Material materials with Níquel of 0.02 % |
Silicona | 0.02 % Show Material materials with Silicona of 0.02 % |
Titanio | 0.08 % Show Material materials with Titanio of 0.08 % |
Vanadio | 0.08 % Show Material materials with Vanadio of 0.08 % |