EN 10292 Grade HX380LAD +Z, +ZF, +ZA, +AZ, +AS,hot rolled or cold rolled, hot dip coated

View suppliers (4)
Want to keep this datasheet? Save it now in your required format

Description

The steel HX380LAD (X=roll condition, LA=low alloyed, D=hot-dip coatable) is producible with the following coatings: - HX380LA+Z (plating Zn) with coating weights (double-sided) of 100, 140, 200, 225 and 275 g/m² (100 g approximate 7,1 µm per side) - HX380LAD+ZF (plating Zn-Fe) with coating weights (double-sided) of 100 and 120 g/m² (100 g approximate 7,1 µm per side) - HX380LAD+ZA (plating Zn-Al) with coating weights (double-sided) of 095, 130, 185, 200 and 255 g/m² (95 g approximate 7,2 µm per side) - HX380LAD+AZ (plating Al-Zn) with coating weights (double-sided) of 100, 150 and 185 g/m² (100 g approximate 13,3 µm per side) - HX380LAD+AS (plating Al-Si) with coating weights (double-sided) of 060 and 080 g/m² (100 g approximate 17 µm per side) The hot dip galvanizing refined flat products are available by arrangement on ordering with different coating weights (also per side). Following surface protection types can be delivered: chemical passivated, oiled, chemical passivated and oiled, sealed, phosphated, phosphated and oiled. Mechanical properties are warranted for a period of 3 months for Bake-hardening steels and for a period of 6 months after provision of the products for all other sorts. The same terms are valid for freedom from stretcher strains (surface type B and C). It is suitable for usual welding methods. For higher coating weights on welding are where approppriate necessary special measures. Furthermore suitability for joining by sticking as well as for application of organic coatings. Application: household appliances industry, construction trade, electrical industry, furniture industry, car industry.,The steel HX380LAD (X=roll condition, LA=low alloyed, D=hot-dip coatable) is deliverable with the following coatings: - HX380LA+Z (plating Zn) with coating weights (double-sided) of 100, 140, 200, 225 and 275 g/m² (100 g approximate 7,1 µm per side) - HX380LAD+ZF (plating Zn-Fe) with coating weights (double-sided) of 100 and 120 g/m² (100 g approximate 7,1 µm per side) - HX380LAD+ZA (plating Zn-Al) with coating weights (double-sided) of 095, 130, 185, 200 and 255 g/m² (95 g approximate 7,2 µm per side) - HX380LAD+AZ (plating Al-Zn) with coating weights (double-sided) of 100, 150 and 185 g/m² (100 g approximate 13,3 µm per side) - HX380LAD+AS (plating Al-Si) with coating weights (double-sided) of 060 and 080 g/m² (100 g approximate 17 µm per side) The hot dip galvanizing refined flat products are available by arrangement on ordering with different coating weights (also per side). Following surface protection types can be delivered: chemical passivated, oiled, chemical passivated and oiled, sealed, phosphated, phosphated and oiled. Mechanical properties are warranted for a period of 6 months after provision. The same time is valid for freedom from stretcher strains (surface type B and C). It is suitable for usual welding methods. For higher coating weights on welding are where approppriate necessary special measures. Furthermore suitability for joining by sticking as well as for application of organic coatings. Application: household appliances industry, construction trade, electrical industry, furniture industry, car industry.

Related Standards

Los datos sobre este material han sido proporcionados por WIAM.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

Propiedades

Mecánica

PropertyTemperatureValue

Elongación A80

20.0 °C

20 %

Show Material materials with Elongación A80 of 20 %

Elongación A80 transversal

20.0 °C

19 %

Show Material materials with Elongación A80 transversal of 19 %

Límite elástico Rp 0,2

20.0 °C

360 - 460 MPa

Show Material materials with Límite elástico Rp 0,2 of 360 - 460 MPa

Límite elástico transversal Rp 0,2

20.0 °C

380 - 480 MPa

Show Material materials with Límite elástico transversal Rp 0,2 of 380 - 480 MPa

Resistencia a la tracción

20.0 °C

430 - 550 MPa

Show Material materials with Resistencia a la tracción of 430 - 550 MPa

Resistencia a la tracción transversal

20.0 °C

440 - 560 MPa

Show Material materials with Resistencia a la tracción transversal of 440 - 560 MPa

Chemical properties

PropertyValue

Aluminio

0.02 %

Show Material materials with Aluminio of 0.02 %

Azufre

0.025 %

Show Material materials with Azufre of 0.025 %

Carbono

0.11 %

Show Material materials with Carbono of 0.11 %

Fósforo

0.03 %

Show Material materials with Fósforo of 0.03 %

Manganeso

1.4 %

Show Material materials with Manganeso of 1.4 %

Niobio

0.09 %

Show Material materials with Niobio of 0.09 %

Silicona

0.5 %

Show Material materials with Silicona of 0.5 %

Titanio

0.15 %