General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.95 g/cm³ Show Material materials with Densidad of 8.95 g/cm³ | Typical for Wrought Copper Nickel Grade |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Hardness, Rockwell Superficial 30-T | 23.0 °C | 45 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 45 [-] | |
Límite elástico Rp0.5 | 23.0 °C | 90 MPa Show Material materials with Límite elástico Rp0.5 of 90 MPa | |
Módulo elástico | 23.0 °C | 120 - 156 GPa Show Material materials with Módulo elástico of 120 - 156 GPa | Typical for Wrought Copper Nickel Grade |
Resistencia a la tracción | 23.0 °C | 260 MPa Show Material materials with Resistencia a la tracción of 260 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 375 - 398 J/(kg·K) Show Material materials with Calor específico of 375 - 398 J/(kg·K) | Typical for Wrought Copper Nickel Grade |
Coeficiente de dilatación térmica | 23.0 °C | 1.4E-5 - 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.4E-5 - 1.8E-5 1/K | Typical for Wrought Copper Nickel Grade |
Conductividad térmica | 23.0 °C | 21 - 195 W/(m·K) Show Material materials with Conductividad térmica of 21 - 195 W/(m·K) | Typical for Wrought Copper Nickel Grade |
Temperatura de fusión | 915 - 1240 °C Show Material materials with Temperatura de fusión of 915 - 1240 °C | Typical for Wrought Copper Nickel Grade |
Chemical properties