General
Property | Value | Comment |
---|---|---|
Densidad | 2.65 - 2.71 g/cm³ Show Material materials with Densidad of 2.65 - 2.71 g/cm³ | Typical for Cast 4xx.x Series Aluminium |
Mecánica
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 4xx.x Series Aluminium | ||
Elongación | 3.5 % Show Material materials with Elongación of 3.5 % | ASTM B85 | Casting | |
Módulo elástico | 71.0 - 75.0 GPa Show Material materials with Módulo elástico of 71.0 - 75.0 GPa | Typical for Cast 4xx.x Series Aluminium | ||
Resistencia a la tracción | 290.0 MPa Show Material materials with Resistencia a la tracción of 290.0 MPa | ASTM B85 | Casting | |
Resistencia al cizallamiento | 170.0 MPa Show Material materials with Resistencia al cizallamiento of 170.0 MPa | ASTM B85 | Casting |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 963.0 J/(kg·K) Show Material materials with Calor específico of 963.0 J/(kg·K) | Typical for Cast 4xx.x Series Aluminium |
Coeficiente de dilatación térmica | 2e-05 - 2.2e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2e-05 - 2.2e-05 1/K | Typical for Cast 4xx.x Series Aluminium |
Conductividad térmica | 130.0 - 170.0 W/(m·K) Show Material materials with Conductividad térmica of 130.0 - 170.0 W/(m·K) | Typical for Cast 4xx.x Series Aluminium |
Temperatura de fusión | 565.0 - 630.0 °C Show Material materials with Temperatura de fusión of 565.0 - 630.0 °C | Typical for Cast 4xx.x Series Aluminium |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Cobre | 1.0 Show Material materials with Cobre of 1.0 | ASTM B85 | Casting |
Estaño | 0.15 Show Material materials with Estaño of 0.15 | ASTM B85 | Casting |
Hierro | 1.3 Show Material materials with Hierro of 1.3 | ASTM B85 | Casting |
Magnesio | 0.1 Show Material materials with Magnesio of 0.1 | ASTM B85 | Casting |
Manganeso | 0.35 Show Material materials with Manganeso of 0.35 | ASTM B85 | Casting |
Níquel | 0.5 Show Material materials with Níquel of 0.5 | ASTM B85 | Casting |
Silicona | 11.0 - 13.0 % Show Material materials with Silicona of 11.0 - 13.0 % | ASTM B85 | Casting |
Zinc | 0.5 Show Material materials with Zinc of 0.5 | ASTM B85 | Casting |