General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7 g/cm³ Show Material materials with Densidad of 7 g/cm³ | Typical for Cast/Wrought Aluminium Zinc Grade |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Magnesium |
Elongación A50 | 23.0 °C | 6 % Show Material materials with Elongación A50 of 6 % | |
Límite elástico Rp 0,2 | 23.0 °C | 131 MPa Show Material materials with Límite elástico Rp 0,2 of 131 MPa | |
Módulo de cizallamiento | 23.0 °C | 45 GPa Show Material materials with Módulo de cizallamiento of 45 GPa | Typical for Magnesium |
Módulo elástico | 23.0 °C | 40 - 45 GPa Show Material materials with Módulo elástico of 40 - 45 GPa | Typical for Cast/Wrought Aluminium Zinc Grade |
Resistencia a la tracción | 23.0 °C | 234 MPa Show Material materials with Resistencia a la tracción of 234 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 800 - 1100 J/(kg·K) Show Material materials with Calor específico of 800 - 1100 J/(kg·K) | Typical for Cast/Wrought Aluminium Zinc Grade |
Coeficiente de dilatación térmica | 23.0 °C | 2.5E-5 - 2.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.5E-5 - 2.6E-5 1/K | Typical for Cast/Wrought Aluminium Zinc Grade |
Conductividad térmica | 23.0 °C | 44 - 110 W/(m·K) Show Material materials with Conductividad térmica of 44 - 110 W/(m·K) | Typical for Cast/Wrought Aluminium Zinc Grade |
Temperatura de fusión | 365 - 645 °C Show Material materials with Temperatura de fusión of 365 - 645 °C | Typical for Cast/Wrought Aluminium Zinc Grade |
Chemical properties
Property | Value |
---|---|
Aluminio | 2.5 - 3.5 % Show Material materials with Aluminio of 2.5 - 3.5 % |
Calcio | 0.04 % Show Material materials with Calcio of 0.04 % |
Cobre | 0.05 % Show Material materials with Cobre of 0.05 % |
Hierro | 5E-3 % Show Material materials with Hierro of 5E-3 % |
Manganeso | 0.2 - 1 % Show Material materials with Manganeso of 0.2 - 1 % |
Níquel | 5E-3 % Show Material materials with Níquel of 5E-3 % |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |
Zinc | 0.6 - 1.4 % Show Material materials with Zinc of 0.6 - 1.4 % |