General
Property | Value | Comment |
---|---|---|
Densidad | 2.65 - 2.71 g/cm³ Show Material materials with Densidad of 2.65 - 2.71 g/cm³ | Typical for Cast 4xx.x Series Aluminium |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 4xx.x Series Aluminium | |||
Dureza Brinell | 45.0 [-] Show Material materials with Dureza Brinell of 45.0 [-] | F; | ASTM B108 | Casting | |
Elongación | 2.5 % Show Material materials with Elongación of 2.5 % | F; | ASTM B108 | Casting | |
Módulo elástico | 71.0 - 75.0 GPa Show Material materials with Módulo elástico of 71.0 - 75.0 GPa | Typical for Cast 4xx.x Series Aluminium | |||
Resistencia a la tracción | 145.0 MPa Show Material materials with Resistencia a la tracción of 145.0 MPa | F; | ASTM B108 | Casting |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 963.0 J/(kg·K) Show Material materials with Calor específico of 963.0 J/(kg·K) | Typical for Cast 4xx.x Series Aluminium |
Coeficiente de dilatación térmica | 2e-05 - 2.2e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2e-05 - 2.2e-05 1/K | Typical for Cast 4xx.x Series Aluminium |
Conductividad térmica | 130.0 - 170.0 W/(m·K) Show Material materials with Conductividad térmica of 130.0 - 170.0 W/(m·K) | Typical for Cast 4xx.x Series Aluminium |
Temperatura de fusión | 565.0 - 630.0 °C Show Material materials with Temperatura de fusión of 565.0 - 630.0 °C | Typical for Cast 4xx.x Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.15 Show Material materials with Cobre of 0.15 | F; | ASTM B108 | Casting |
Hierro | 0.8 Show Material materials with Hierro of 0.8 | F; | ASTM B108 | Casting |
Magnesio | 0.05 Show Material materials with Magnesio of 0.05 | F; | ASTM B108 | Casting |
Manganeso | 0.35 Show Material materials with Manganeso of 0.35 | F; | ASTM B108 | Casting |
Silicona | 4.5 - 6.0 % Show Material materials with Silicona of 4.5 - 6.0 % | F; | ASTM B108 | Casting |
Titanio | 0.25 Show Material materials with Titanio of 0.25 | F; | ASTM B108 | Casting |
Zinc | 0.35 Show Material materials with Zinc of 0.35 | F; | ASTM B108 | Casting |