General
Property | Value | Comment |
---|---|---|
Densidad | 2.8 g/cm³ Show Material materials with Densidad of 2.8 g/cm³ | Typical for Cast 7xx.x Series Aluminium |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 7xx.x Series Aluminium | |||
Elongación | 9.0 % Show Material materials with Elongación of 9.0 % | T1 or T5 | ASTM B108 | Casting | |
Módulo elástico | 74.0 GPa Show Material materials with Módulo elástico of 74.0 GPa | Typical for Cast 7xx.x Series Aluminium | |||
Resistencia a la tracción | 255.0 MPa Show Material materials with Resistencia a la tracción of 255.0 MPa | T1 or T5 | ASTM B108 | Casting |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 963.0 J/(kg·K) Show Material materials with Calor específico of 963.0 J/(kg·K) | Typical for Cast 7xx.x Series Aluminium |
Coeficiente de dilatación térmica | 2.4e-05 - 2.5e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.4e-05 - 2.5e-05 1/K | Typical for Cast 7xx.x Series Aluminium |
Conductividad térmica | 100.0 - 160.0 W/(m·K) Show Material materials with Conductividad térmica of 100.0 - 160.0 W/(m·K) | Typical for Cast 7xx.x Series Aluminium |
Temperatura de fusión | 550.0 - 645.0 °C Show Material materials with Temperatura de fusión of 550.0 - 645.0 °C | Typical for Cast 7xx.x Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.2 Show Material materials with Cobre of 0.2 | T1 or T5 | ASTM B108 | Casting |
Cromo | 0.2 - 0.4 % Show Material materials with Cromo of 0.2 - 0.4 % | T1 or T5 | ASTM B108 | Casting |
Hierro | 0.8 Show Material materials with Hierro of 0.8 | T1 or T5 | ASTM B108 | Casting |
Magnesio | 1.4 - 1.8 % Show Material materials with Magnesio of 1.4 - 1.8 % | T1 or T5 | ASTM B108 | Casting |
Manganeso | 0.4 - 0.6 % Show Material materials with Manganeso of 0.4 - 0.6 % | T1 or T5 | ASTM B108 | Casting |
Silicona | 0.2 Show Material materials with Silicona of 0.2 | T1 or T5 | ASTM B108 | Casting |
Titanio | 0.25 Show Material materials with Titanio of 0.25 | T1 or T5 | ASTM B108 | Casting |
Zinc | 2.7 - 3.3 % Show Material materials with Zinc of 2.7 - 3.3 % | T1 or T5 | ASTM B108 | Casting |