General
Property | Value | Comment |
---|---|---|
Densidad | 2.8 g/cm³ Show Material materials with Densidad of 2.8 g/cm³ | Typical for Cast 8xx.x Series Aluminium |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 8xx.x Series Aluminium | |||
Elongación | 3.0 % Show Material materials with Elongación of 3.0 % | T5 | ASTM B108 | Casting | |
Módulo elástico | 70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | Typical for Cast 8xx.x Series Aluminium | |||
Resistencia a la tracción | 115.0 MPa Show Material materials with Resistencia a la tracción of 115.0 MPa | T5 | ASTM B108 | Casting |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 963.0 J/(kg·K) Show Material materials with Calor específico of 963.0 J/(kg·K) | Typical for Cast 8xx.x Series Aluminium |
Coeficiente de dilatación térmica | 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3e-05 1/K | Typical for Cast 8xx.x Series Aluminium |
Temperatura de fusión | 205.0 - 650.0 °C Show Material materials with Temperatura de fusión of 205.0 - 650.0 °C | Typical for Cast 8xx.x Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.7 - 1.3 % Show Material materials with Cobre of 0.7 - 1.3 % | T5 | ASTM B108 | Casting |
Estaño | 5.5 - 7.0 % Show Material materials with Estaño of 5.5 - 7.0 % | T5 | ASTM B108 | Casting |
Hierro | 0.7 Show Material materials with Hierro of 0.7 | T5 | ASTM B108 | Casting |
Magnesio | 0.1 Show Material materials with Magnesio of 0.1 | T5 | ASTM B108 | Casting |
Manganeso | 0.1 Show Material materials with Manganeso of 0.1 | T5 | ASTM B108 | Casting |
Níquel | 0.3 - 0.7 % Show Material materials with Níquel of 0.3 - 0.7 % | T5 | ASTM B108 | Casting |
Silicona | 2.0 - 3.0 % Show Material materials with Silicona of 2.0 - 3.0 % | T5 | ASTM B108 | Casting |
Titanio | 0.2 Show Material materials with Titanio of 0.2 | T5 | ASTM B108 | Casting |