General
Property | Value | Comment |
---|---|---|
Densidad | 2.7 g/cm³ Show Material materials with Densidad of 2.7 g/cm³ | Typical for Wrought 1000 Series Aluminium |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 1000 Series Aluminium | |||
Elongación | 22.0 % Show Material materials with Elongación of 22.0 % | O | ASTM B211 | Bar, Rod, Wire | |
25.0 % Show Material materials with Elongación of 25.0 % | O | ASTM B211 | Bar, Rod, Wire | A50 | |
Módulo de cizallamiento | 25.9 GPa Show Material materials with Módulo de cizallamiento of 25.9 GPa | Typical for Wrought 1000 Series Aluminium | |||
Módulo elástico | 68.0 - 70.0 GPa Show Material materials with Módulo elástico of 68.0 - 70.0 GPa | Typical for Wrought 1000 Series Aluminium | |||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 1000 Series Aluminium | |||
Resistencia a la tracción | 75.0 - 105.0 MPa Show Material materials with Resistencia a la tracción of 75.0 - 105.0 MPa | O | ASTM B211 | Bar, Rod, Wire |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 900.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 900.0 - 963.0 J/(kg·K) | Typical for Wrought 1000 Series Aluminium |
Coeficiente de dilatación térmica | 2.2e-05 - 2.5e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.2e-05 - 2.5e-05 1/K | Typical for Wrought 1000 Series Aluminium |
Conductividad térmica | 167.0 - 244.0 W/(m·K) Show Material materials with Conductividad térmica of 167.0 - 244.0 W/(m·K) | Typical for Wrought 1000 Series Aluminium |
Temperatura de fusión | 645.0 - 660.0 °C Show Material materials with Temperatura de fusión of 645.0 - 660.0 °C | Typical for Wrought 1000 Series Aluminium |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 33000000.0 - 38000000.0 S/m Show Material materials with Conductividad eléctrica of 33000000.0 - 38000000.0 S/m | Typical for Wrought 1000 Series Aluminium |
Resistividad eléctrica | 2.7e-08 - 3e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.7e-08 - 3e-08 Ω·m | Typical for Wrought 1000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 99.0 % Show Material materials with Aluminio of 99.0 % | O | ASTM B211 | Bar, Rod, Wire |
Cobre | 0.05 - 0.2 % Show Material materials with Cobre of 0.05 - 0.2 % | O | ASTM B211 | Bar, Rod, Wire |
Manganeso | 0.05 Show Material materials with Manganeso of 0.05 | O | ASTM B211 | Bar, Rod, Wire |
Zinc | 0.1 Show Material materials with Zinc of 0.1 | O | ASTM B211 | Bar, Rod, Wire |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent | |
Workability | Excellent workability. |