General
Property | Value | Comment |
---|---|---|
Densidad | 2.75 - 2.84 g/cm³ Show Material materials with Densidad of 2.75 - 2.84 g/cm³ | Typical for Wrought 2000 Series Aluminium |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 2000 Series Aluminium | |||
Elongación | 5.0 % Show Material materials with Elongación of 5.0 % | T81, T8510, T8511; Area through 16000 mm2 | ASTM B241 | Tube | |
6.0 % Show Material materials with Elongación of 6.0 % | T81, T8510, T8511; Area through 16000 mm2 | ASTM B241 | Tube | A50 | |
Módulo de cizallamiento | 26.0 - 27.5 GPa Show Material materials with Módulo de cizallamiento of 26.0 - 27.5 GPa | Typical for Wrought 2000 Series Aluminium | |||
Módulo elástico | 70.0 - 73.0 GPa Show Material materials with Módulo elástico of 70.0 - 73.0 GPa | Typical for Wrought 2000 Series Aluminium | |||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 2000 Series Aluminium | |||
Resistencia a la tracción | 400.0 MPa Show Material materials with Resistencia a la tracción of 400.0 MPa | T81, T8510, T8511; Area through 16000 mm2 | ASTM B241 | Tube |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 816.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 816.0 - 963.0 J/(kg·K) | Typical for Wrought 2000 Series Aluminium |
Coeficiente de dilatación térmica | 1.6e-05 - 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6e-05 - 2.4e-05 1/K | Typical for Wrought 2000 Series Aluminium |
Conductividad térmica | 112.0 - 251.0 W/(m·K) Show Material materials with Conductividad térmica of 112.0 - 251.0 W/(m·K) | Typical for Wrought 2000 Series Aluminium |
Temperatura de fusión | 500.0 - 650.0 °C Show Material materials with Temperatura de fusión of 500.0 - 650.0 °C | Typical for Wrought 2000 Series Aluminium |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 18000000.0 - 30000000.0 S/m Show Material materials with Conductividad eléctrica of 18000000.0 - 30000000.0 S/m | Typical for Wrought 2000 Series Aluminium |
Resistividad eléctrica | 3.4e-08 - 6e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.4e-08 - 6e-08 Ω·m | Typical for Wrought 2000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 5.8 - 6.8 % Show Material materials with Cobre of 5.8 - 6.8 % | T81, T8510, T8511; Area through 16000 mm2 | ASTM B241 | Tube |
Hierro | 0.3 Show Material materials with Hierro of 0.3 | T81, T8510, T8511; Area through 16000 mm2 | ASTM B241 | Tube |
Magnesio | 0.02 Show Material materials with Magnesio of 0.02 | T81, T8510, T8511; Area through 16000 mm2 | ASTM B241 | Tube |
Manganeso | 0.2 - 0.4 % Show Material materials with Manganeso of 0.2 - 0.4 % | T81, T8510, T8511; Area through 16000 mm2 | ASTM B241 | Tube |
Silicona | 0.2 Show Material materials with Silicona of 0.2 | T81, T8510, T8511; Area through 16000 mm2 | ASTM B241 | Tube |
Titanio | 0.02 - 0.1 % Show Material materials with Titanio of 0.02 - 0.1 % | T81, T8510, T8511; Area through 16000 mm2 | ASTM B241 | Tube |
Zinc | 0.1 Show Material materials with Zinc of 0.1 | T81, T8510, T8511; Area through 16000 mm2 | ASTM B241 | Tube |
Technological properties
Property | ||
---|---|---|
Workability | Moderate Workability |