General
Property | Value | Comment |
---|---|---|
Densidad | 2.7 - 2.85 g/cm³ Show Material materials with Densidad of 2.7 - 2.85 g/cm³ | Typical for Wrought 7000 Series Aluminium |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 7000 Series Aluminium | |||
Elongación | 9.0 % Show Material materials with Elongación of 9.0 % | T73 | ASTM B316 | Wire, Rod | |
Módulo de cizallamiento | 26.4 - 27.1 GPa Show Material materials with Módulo de cizallamiento of 26.4 - 27.1 GPa | Typical for Wrought 7000 Series Aluminium | |||
Módulo elástico | 69.0 - 72.0 GPa Show Material materials with Módulo elástico of 69.0 - 72.0 GPa | Typical for Wrought 7000 Series Aluminium | |||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 7000 Series Aluminium | |||
Resistencia a la tracción | 470.0 MPa Show Material materials with Resistencia a la tracción of 470.0 MPa | T73 | ASTM B316 | Wire, Rod | |
Resistencia al cizallamiento | 280.0 MPa Show Material materials with Resistencia al cizallamiento of 280.0 MPa | T73 | ASTM B316 | Wire, Rod |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 795.0 - 1050.0 J/(kg·K) Show Material materials with Calor específico of 795.0 - 1050.0 J/(kg·K) | Typical for Wrought 7000 Series Aluminium |
Coeficiente de dilatación térmica | 2.1e-05 - 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.1e-05 - 2.4e-05 1/K | Typical for Wrought 7000 Series Aluminium |
Conductividad térmica | 121.0 - 170.0 W/(m·K) Show Material materials with Conductividad térmica of 121.0 - 170.0 W/(m·K) | Typical for Wrought 7000 Series Aluminium |
Temperatura de fusión | 465.0 - 655.0 °C Show Material materials with Temperatura de fusión of 465.0 - 655.0 °C | Typical for Wrought 7000 Series Aluminium |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 18000000.0 - 34000000.0 S/m Show Material materials with Conductividad eléctrica of 18000000.0 - 34000000.0 S/m | Typical for Wrought 7000 Series Aluminium |
Resistividad eléctrica | 2.9e-08 - 5.6e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.9e-08 - 5.6e-08 Ω·m | Typical for Wrought 7000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 1.2 - 2.0 % Show Material materials with Cobre of 1.2 - 2.0 % | T73 | ASTM B316 | Wire, Rod |
Cromo | 0.18 - 0.28 % Show Material materials with Cromo of 0.18 - 0.28 % | T73 | ASTM B316 | Wire, Rod |
Hierro | 0.5 Show Material materials with Hierro of 0.5 | T73 | ASTM B316 | Wire, Rod |
Magnesio | 2.1 - 2.9 % Show Material materials with Magnesio of 2.1 - 2.9 % | T73 | ASTM B316 | Wire, Rod |
Manganeso | 0.3 Show Material materials with Manganeso of 0.3 | T73 | ASTM B316 | Wire, Rod |
Silicona | 0.4 Show Material materials with Silicona of 0.4 | T73 | ASTM B316 | Wire, Rod |
Titanio | 0.2 Show Material materials with Titanio of 0.2 | T73 | ASTM B316 | Wire, Rod |
Zinc | 5.1 - 6.1 % Show Material materials with Zinc of 5.1 - 6.1 % | T73 | ASTM B316 | Wire, Rod |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent |