Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 201 - 255 [-] Show Material materials with Dureza Brinell of 201 - 255 [-] |
Elongación | 20.0 °C | 15 - 17 % Show Material materials with Elongación of 15 - 17 % |
Límite elástico | 20.0 °C | 495 - 525 MPa Show Material materials with Límite elástico of 495 - 525 MPa |
Límite elástico Rp 0,2 | 20.0 °C | 480 - 510 MPa Show Material materials with Límite elástico Rp 0,2 of 480 - 510 MPa |
Resistencia a la tracción | 20.0 °C | 700 - 850 MPa Show Material materials with Resistencia a la tracción of 700 - 850 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.04 % Show Material materials with Azufre of 0.04 % |
Carbono | 0.32 - 0.4 % Show Material materials with Carbono of 0.32 - 0.4 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Hierro | Balance |
Manganeso | 1.3 - 1.7 % Show Material materials with Manganeso of 1.3 - 1.7 % |
Molibdeno | 0.22 - 0.32 % Show Material materials with Molibdeno of 0.22 - 0.32 % |
Silicona | 0.1 - 0.4 % Show Material materials with Silicona of 0.1 - 0.4 % |