Molybdenum Steel
EN 10028-2 Grade 16Mo3 normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Nickel molybdenum Steel
EN 10028-2 Grade 15NiCuMoNb5-6-4 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10025-5 Grade S355J2W normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10025-5 Grade S355K2W normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10225 Grade S420G1 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Acero bajo en carbono
ASTM A841 Grade B Class 1 Thermo-Mechanical Control Process (TMCP)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-6 Grade P355Q quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-6 Grade P355QH quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-6 Grade P355QL1 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-6 Grade P355QL2 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10225 Grade S420G1 thermomechanically rolledSuministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10225 Grade S460G1 thermomechanically rolledSuministrada por:
1 proveedor Matmatch
Chromium Molybdenum Steel
ASTM A829 Grade 4142 As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPaSuministrada por:
1 proveedor Matmatch
Chromium Molybdenum Steel
ASTM A829 Grade 4140 As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPaSuministrada por:
1 proveedor Matmatch
Unclassified Stainless Steel
ASTM A543 Class 1 Type B Quenched and TemperedSuministrada por:
1 proveedor Matmatch
Unclassified Stainless Steel
ASTM A543 Class 1 Type C Quenched and TemperedSuministrada por:
1 proveedor Matmatch
Nickel Chromium Molybdenum Steel
Carbodur 6587 Blank HardenedSuministrada por:
Deutsche Edelstahlwerke (DEW)