DIN 17182 Grade G13MnNi6-4 quenched and tempered (+QT)

Want to keep this datasheet? Save it now in your required format

Description

In comparison to the unalloyed cast steel grades according to DIN 1681, the materials of this group show distinctly higher values of the notch impact energy. As a result of their low carbon content (0.23 per cent maximum), they are well suitable for welding. The material GS-13 MnNi 6 4, which was developed especially for the offshore-application, ensures problem-free weldability for greater wall thicknesses, too, and it distinguishes itself by a high endurance limit, i.e. fatigue strength.

Related Standards

Equivalent Materials

Los datos sobre este material han sido proporcionados por WIAM.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValueComment

Densidad

23.0 °C

8.8 g/cm³

Show Material materials with Densidad of 8.8 g/cm³

Typical for Nickel Steel

Mecánica

PropertyTemperatureValueComment

Coeficiente de Poisson

23.0 °C

0.29 [-]

Show Material materials with Coeficiente de Poisson of 0.29 [-]

Typical for Nickel Steel

Elongación

20.0 °C

20 - 22 %

Show Material materials with Elongación of 20 - 22 %

Límite elástico

20.0 °C

300 - 340 MPa

Show Material materials with Límite elástico of 300 - 340 MPa

Módulo de cizallamiento

23.0 °C

76 GPa

Show Material materials with Módulo de cizallamiento of 76 GPa

Typical for Nickel Steel

Módulo elástico

23.0 °C

200 - 215 GPa

Show Material materials with Módulo elástico of 200 - 215 GPa

Typical for Nickel Steel

Resistencia a la tracción

20.0 °C

460 - 630 MPa

Show Material materials with Resistencia a la tracción of 460 - 630 MPa

Aplicaciones térmicas

PropertyTemperatureValueComment

Calor específico

23.0 °C

456 J/(kg·K)

Show Material materials with Calor específico of 456 J/(kg·K)

Typical for Nickel Steel

Conductividad térmica

23.0 °C

10 - 50 W/(m·K)

Show Material materials with Conductividad térmica of 10 - 50 W/(m·K)

Typical for Nickel Steel

Temperatura de fusión

1316 - 1595 °C

Show Material materials with Temperatura de fusión of 1316 - 1595 °C

Typical for Nickel Steel

Chemical properties

PropertyValue

Azufre

0.01 %

Show Material materials with Azufre of 0.01 %

Carbono

0.08 - 0.15 %

Show Material materials with Carbono of 0.08 - 0.15 %

Cromo

0.3 %

Show Material materials with Cromo of 0.3 %

Fósforo

0.02 %

Show Material materials with Fósforo of 0.02 %

Manganeso

1 - 1.7 %

Show Material materials with Manganeso of 1 - 1.7 %

Molibdeno

0.2 %

Show Material materials with Molibdeno of 0.2 %

Niobio

0.05 %

Show Material materials with Niobio of 0.05 %

Nitrógeno

0.02 %

Show Material materials with Nitrógeno of 0.02 %

Níquel

0.8 - 1.2 %

Show Material materials with Níquel of 0.8 - 1.2 %

Silicona

0.6 %

Show Material materials with Silicona of 0.6 %

Vanadio

0.1 %

Show Material materials with Vanadio of 0.1 %