General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.9 g/cm³ Show Material materials with Densidad of 7.9 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Austenitic Stainless Steel |
Dureza Brinell | 20.0 °C | 130 - 200 [-] Show Material materials with Dureza Brinell of 130 - 200 [-] | |
Elongación | 20.0 °C | 20 % Show Material materials with Elongación of 20 % | |
Límite elástico Rp 0,2 | 20.0 °C | 175 MPa Show Material materials with Límite elástico Rp 0,2 of 175 MPa | |
100.0 °C | 150 MPa Show Material materials with Límite elástico Rp 0,2 of 150 MPa | ||
150.0 °C | 135 MPa Show Material materials with Límite elástico Rp 0,2 of 135 MPa | ||
200.0 °C | 130 MPa Show Material materials with Límite elástico Rp 0,2 of 130 MPa | ||
250.0 °C | 125 MPa Show Material materials with Límite elástico Rp 0,2 of 125 MPa | ||
300.0 °C | 120 MPa Show Material materials with Límite elástico Rp 0,2 of 120 MPa | ||
350.0 °C | 115 MPa Show Material materials with Límite elástico Rp 0,2 of 115 MPa | ||
400.0 °C | 110 MPa Show Material materials with Límite elástico Rp 0,2 of 110 MPa | ||
450.0 °C | 105 MPa Show Material materials with Límite elástico Rp 0,2 of 105 MPa | ||
500.0 °C | 100 MPa Show Material materials with Límite elástico Rp 0,2 of 100 MPa | ||
550.0 °C | 90 MPa Show Material materials with Límite elástico Rp 0,2 of 90 MPa | ||
Límite elástico Rp 1,0 | 20.0 °C | 200 MPa Show Material materials with Límite elástico Rp 1,0 of 200 MPa | |
100.0 °C | 175 MPa Show Material materials with Límite elástico Rp 1,0 of 175 MPa | ||
150.0 °C | 160 MPa Show Material materials with Límite elástico Rp 1,0 of 160 MPa | ||
200.0 °C | 155 MPa Show Material materials with Límite elástico Rp 1,0 of 155 MPa | ||
250.0 °C | 150 MPa Show Material materials with Límite elástico Rp 1,0 of 150 MPa | ||
300.0 °C | 145 MPa Show Material materials with Límite elástico Rp 1,0 of 145 MPa | ||
350.0 °C | 140 MPa Show Material materials with Límite elástico Rp 1,0 of 140 MPa | ||
400.0 °C | 130 MPa Show Material materials with Límite elástico Rp 1,0 of 130 MPa | ||
450.0 °C | 120 MPa Show Material materials with Límite elástico Rp 1,0 of 120 MPa | ||
500.0 °C | 110 MPa Show Material materials with Límite elástico Rp 1,0 of 110 MPa | ||
550.0 °C | 100 MPa Show Material materials with Límite elástico Rp 1,0 of 100 MPa | ||
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Austenitic Stainless Steel |
Módulo elástico | 23.0 °C | 195 GPa Show Material materials with Módulo elástico of 195 GPa | Typical for Austenitic Stainless Steel |
Resistencia a la tracción | 20.0 °C | 440 - 640 MPa Show Material materials with Resistencia a la tracción of 440 - 640 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 500 J/(kg·K) Show Material materials with Calor específico of 500 J/(kg·K) | |
Coeficiente de dilatación térmica | 100.0 °C | 1.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 1/K | |
200.0 °C | 1.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 1/K | ||
300.0 °C | 1.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 1/K | ||
400.0 °C | 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.8E-5 1/K | ||
500.0 °C | 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.8E-5 1/K | ||
Conductividad térmica | 20.0 °C | 15 W/(m·K) Show Material materials with Conductividad térmica of 15 W/(m·K) | |
Temperatura de fusión | 1230 - 1480 °C Show Material materials with Temperatura de fusión of 1230 - 1480 °C | Typical for Austenitic Stainless Steel | |
Temperatura máx. de funcionamiento, largo | 0 - 550 °C Show Material materials with Temperatura máx. de funcionamiento, largo of 0 - 550 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 5.5E-7 - 7.5E-7 Ω·m Show Material materials with Resistividad eléctrica of 5.5E-7 - 7.5E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.06 % Show Material materials with Carbono of 0.06 % |
Cromo | 18 - 20 % Show Material materials with Cromo of 18 - 20 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Manganeso | 1.5 % Show Material materials with Manganeso of 1.5 % |
Níquel | 9 - 11 % Show Material materials with Níquel of 9 - 11 % |
Silicona | 1.5 % Show Material materials with Silicona of 1.5 % |