General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.7 - 7.76 g/cm³ Show Material materials with Densidad of 7.7 - 7.76 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.28 [-] Show Material materials with Coeficiente de Poisson of 0.28 [-] |
Dureza Brinell | 20.0 °C | 220 - 280 [-] Show Material materials with Dureza Brinell of 220 - 280 [-] |
Elongación | 20.0 °C | 14 % Show Material materials with Elongación of 14 % |
Elongación transversal | 20.0 °C | 10 % Show Material materials with Elongación transversal of 10 % |
Hardness, Brinell, trans | 20.0 °C | 220 - 280 [-] Show Material materials with Hardness, Brinell, trans of 220 - 280 [-] |
Límite elástico | 20.0 °C | 550 MPa Show Material materials with Límite elástico of 550 MPa |
Límite elástico Rp 0,2 | 50.0 °C | 530 MPa Show Material materials with Límite elástico Rp 0,2 of 530 MPa |
100.0 °C | 520 MPa Show Material materials with Límite elástico Rp 0,2 of 520 MPa | |
150.0 °C | 510 MPa Show Material materials with Límite elástico Rp 0,2 of 510 MPa | |
200.0 °C | 500 MPa Show Material materials with Límite elástico Rp 0,2 of 500 MPa | |
250.0 °C | 420 MPa Show Material materials with Límite elástico Rp 0,2 of 420 MPa | |
300.0 °C | 480 MPa Show Material materials with Límite elástico Rp 0,2 of 480 MPa | |
350.0 °C | 450 MPa Show Material materials with Límite elástico Rp 0,2 of 450 MPa | |
400.0 °C | 410 MPa Show Material materials with Límite elástico Rp 0,2 of 410 MPa | |
Límite elástico transversal | 20.0 °C | 550 MPa Show Material materials with Límite elástico transversal of 550 MPa |
Módulo de cizallamiento | 20.0 °C | 84.95 GPa Show Material materials with Módulo de cizallamiento of 84.95 GPa |
Módulo elástico | 20.0 °C | 217.68 - 220 GPa Show Material materials with Módulo elástico of 217.68 - 220 GPa |
100.0 °C | 213 - 216 GPa Show Material materials with Módulo elástico of 213 - 216 GPa | |
200.0 °C | 206 - 209 GPa Show Material materials with Módulo elástico of 206 - 209 GPa | |
300.0 °C | 198 - 200 GPa Show Material materials with Módulo elástico of 198 - 200 GPa | |
400.0 °C | 190 - 192 GPa Show Material materials with Módulo elástico of 190 - 192 GPa | |
500.0 °C | 180 - 183 GPa Show Material materials with Módulo elástico of 180 - 183 GPa | |
600.0 °C | 167 GPa Show Material materials with Módulo elástico of 167 GPa | |
Resistencia a la tracción | 20.0 °C | 750 - 900 MPa Show Material materials with Resistencia a la tracción of 750 - 900 MPa |
Resistencia a la tracción transversal | 20.0 °C | 750 - 900 MPa Show Material materials with Resistencia a la tracción transversal of 750 - 900 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 430 - 439 J/(kg·K) Show Material materials with Calor específico of 430 - 439 J/(kg·K) | |
100.0 °C | 474 J/(kg·K) Show Material materials with Calor específico of 474 J/(kg·K) | ||
200.0 °C | 498 J/(kg·K) Show Material materials with Calor específico of 498 J/(kg·K) | ||
300.0 °C | 517 J/(kg·K) Show Material materials with Calor específico of 517 J/(kg·K) | ||
400.0 °C | 538 J/(kg·K) Show Material materials with Calor específico of 538 J/(kg·K) | ||
500.0 °C | 564 J/(kg·K) Show Material materials with Calor específico of 564 J/(kg·K) | ||
600.0 °C | 598 J/(kg·K) Show Material materials with Calor específico of 598 J/(kg·K) | ||
Coeficiente de dilatación térmica | 20.0 °C | 1.02E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.02E-5 1/K | |
100.0 °C | 1.04E-5 - 1.05E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.04E-5 - 1.05E-5 1/K | ||
200.0 °C | 1.08E-5 - 1.09E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.08E-5 - 1.09E-5 1/K | ||
300.0 °C | 1.12E-5 - 1.13E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.12E-5 - 1.13E-5 1/K | ||
400.0 °C | 1.16E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.16E-5 1/K | ||
500.0 °C | 1.19E-5 - 1.2E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.19E-5 - 1.2E-5 1/K | ||
600.0 °C | 1.22E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.22E-5 1/K | ||
Conductividad térmica | 20.0 °C | 24 - 25 W/(m·K) Show Material materials with Conductividad térmica of 24 - 25 W/(m·K) | |
100.0 °C | 24.4 W/(m·K) Show Material materials with Conductividad térmica of 24.4 W/(m·K) | ||
200.0 °C | 24.8 W/(m·K) Show Material materials with Conductividad térmica of 24.8 W/(m·K) | ||
300.0 °C | 25.1 W/(m·K) Show Material materials with Conductividad térmica of 25.1 W/(m·K) | ||
400.0 °C | 25.6 W/(m·K) Show Material materials with Conductividad térmica of 25.6 W/(m·K) | ||
500.0 °C | 26.1 W/(m·K) Show Material materials with Conductividad térmica of 26.1 W/(m·K) | ||
600.0 °C | 26.4 W/(m·K) Show Material materials with Conductividad térmica of 26.4 W/(m·K) | ||
Difusividad térmica | 20.0 °C | 7.1 mm²/s Show Material materials with Difusividad térmica of 7.1 mm²/s | |
100.0 °C | 6.3 mm²/s Show Material materials with Difusividad térmica of 6.3 mm²/s | ||
200.0 °C | 6 mm²/s Show Material materials with Difusividad térmica of 6 mm²/s | ||
300.0 °C | 5.7 mm²/s Show Material materials with Difusividad térmica of 5.7 mm²/s | ||
400.0 °C | 5.4 mm²/s Show Material materials with Difusividad térmica of 5.4 mm²/s | ||
500.0 °C | 4.9 mm²/s Show Material materials with Difusividad térmica of 4.9 mm²/s | ||
600.0 °C | 4.1 mm²/s Show Material materials with Difusividad térmica of 4.1 mm²/s | ||
Temperatura de fusión | 1425 - 1530 °C Show Material materials with Temperatura de fusión of 1425 - 1530 °C | Typical for Ferritic Stainless Steel | |
Temperatura máx. de funcionamiento, largo | 0 - 500 °C Show Material materials with Temperatura máx. de funcionamiento, largo of 0 - 500 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 6.03E-7 Ω·m Show Material materials with Resistividad eléctrica of 6.03E-7 Ω·m |
100.0 °C | 6.68E-7 Ω·m Show Material materials with Resistividad eléctrica of 6.68E-7 Ω·m | |
200.0 °C | 7.43E-7 Ω·m Show Material materials with Resistividad eléctrica of 7.43E-7 Ω·m | |
300.0 °C | 8.17E-7 Ω·m Show Material materials with Resistividad eléctrica of 8.17E-7 Ω·m | |
400.0 °C | 8.9E-7 Ω·m Show Material materials with Resistividad eléctrica of 8.9E-7 Ω·m | |
500.0 °C | 9.62E-7 Ω·m Show Material materials with Resistividad eléctrica of 9.62E-7 Ω·m | |
600.0 °C | 1.04E-6 Ω·m Show Material materials with Resistividad eléctrica of 1.04E-6 Ω·m | |
Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.17 - 0.22 % Show Material materials with Carbono of 0.17 - 0.22 % |
Cromo | 12 - 14 % Show Material materials with Cromo of 12 - 14 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 0.9 - 1.3 % Show Material materials with Molibdeno of 0.9 - 1.3 % |
Níquel | 1 % Show Material materials with Níquel of 1 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |