Nickel Steel
EN 10028-4 Grade X12Ni5 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Nickel Steel
EN 10028-4 Grade 12Ni14 normalized and tempered (+NT)Suministrada por:
1 proveedor Matmatch
Nickel Molybdenum Steel
ASTM A387 Grade 11 Class 1, Annealed, Normalized and Tempered, or Quenched and TemperedSuministrada por:
1 proveedor Matmatch
Acero inoxidable martensítico
ASTM A841 Grade A Class 1 Thermo-Mechanical Control Process (TMCP)Suministrada por:
1 proveedor Matmatch
Aleación de níquel-hierro
Alloy 52 BarAleación de níquel-hierro
Alloy 52 Strip/CoilAcero inoxidable ferrítico
DIN 17440 Grade X6Cr17 soft annealed (+A)Acero inoxidable ferrítico
DIN 17440 Grade X3CrTi17 soft annealed (+A)Acero inoxidable ferrítico
DIN 17440 Grade X6CrAl13 soft annealed (+A)Acero inoxidable ferrítico
EN 10088-1 Grade X3CrNb17 soft annealed (+A)Acero inoxidable martensítico
DIN 17440 Grade X12Cr13 soft annealed (+A)Acero inoxidable ferrítico
SEW 400 Grade X20CrMo13 quenched and tempered (+QT)Acero inoxidable martensítico
EN 10088-1 Grade X6Cr13 soft annealed (+A)Acero inoxidable martensítico
DIN 17440 Grade X20Cr13 quenched and tempered (+QT)Poliéter éter cetona (PEEK)
Polyetheretherketone Reinforced with 30% Carbon Fibre (PEEK+CF30)Suministrada por:
2 proveedores de Matmatch
Polyamide 6 (PA6)
Polyamide 6 Reinforced with 50% Glass Fibers (PA6+GF50)Suministrada por:
2 proveedores de Matmatch
Acero inoxidable ferrítico
EN 10088-1 Grade X6CrAl13 soft annealed (+A)Acero inoxidable ferrítico
EN 10088-1 Grade X6CrMo17-1 soft annealed (+A)Acero inoxidable ferrítico
EN 10088-1 Grade X3CrTi17 soft annealed (+A)