General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.7 g/cm³ Show Material materials with Densidad of 7.7 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Ferritic Stainless Steel |
Dureza Brinell | 20.0 °C | 260 - 330 [-] Show Material materials with Dureza Brinell of 260 - 330 [-] | |
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Ferritic Stainless Steel |
Módulo elástico | 23.0 °C | 220 GPa Show Material materials with Módulo elástico of 220 GPa | Typical for Ferritic Stainless Steel |
Resistencia a la tracción | 20.0 °C | 880 - 1080 MPa Show Material materials with Resistencia a la tracción of 880 - 1080 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 500 J/(kg·K) Show Material materials with Calor específico of 500 J/(kg·K) | |
Coeficiente de dilatación térmica | 100.0 °C | 9.5E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 9.5E-6 1/K | |
200.0 °C | 1E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1E-5 1/K | ||
300.0 °C | 1.05E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.05E-5 1/K | ||
400.0 °C | 1.1E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.1E-5 1/K | ||
500.0 °C | 1.15E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.15E-5 1/K | ||
Conductividad térmica | 20.0 °C | 19 W/(m·K) Show Material materials with Conductividad térmica of 19 W/(m·K) | |
Temperatura de fusión | 1425 - 1530 °C Show Material materials with Temperatura de fusión of 1425 - 1530 °C | Typical for Ferritic Stainless Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 6E-7 - 7.5E-7 Ω·m Show Material materials with Resistividad eléctrica of 6E-7 - 7.5E-7 Ω·m | Typical for Ferritic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.9 - 1.3 % Show Material materials with Carbono of 0.9 - 1.3 % |
Cromo | 27 - 29 % Show Material materials with Cromo of 27 - 29 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 2 - 2.5 % Show Material materials with Molibdeno of 2 - 2.5 % |
Silicona | 2 % Show Material materials with Silicona of 2 % |