Conductividad térmica: 19 W/(m·K)

Quick Comparison

Nickel Chromium Iron Alloy

Sanicro® 28

Suministrada por:

Alleima (formerly Sandvik Materials Technology)

Aleación de níquel-hierro

VDM® Alloy 33

Suministrada por:

VDM Metals

Acero inoxidable austenítico

Esshete 1250

Suministrada por:

Alleima (formerly Sandvik Materials Technology)

Acero inoxidable martensítico

ASTM A841 Grade A Class 1 Thermo-Mechanical Control Process (TMCP)

Suministrada por:

1 proveedor Matmatch

Nickel Steel

ASTM A353 Double-Normalized and Tempered

Suministrada por:

1 proveedor Matmatch

Acero inoxidable austenítico

Sandvik 2RE69

Suministrada por:

Alleima (formerly Sandvik Materials Technology)

Nickel Chromium Iron Alloy

Sanicro 31HT

Suministrada por:

Alleima (formerly Sandvik Materials Technology)

Tin Bronze

ASTM B505 Grade C90700

Suministrada por:

1 proveedor Matmatch

Leaded Tin Bronze

ASTM B505 Grade C92700

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95200

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95300 Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95300 HT, Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95500 Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95500 HT, Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95520

Suministrada por:

1 proveedor Matmatch

Acero inoxidable austenítico

Permodur 4841 +AT

Suministrada por:

Deutsche Edelstahlwerke (DEW)

Acero inoxidable austenítico

Sandvik 2RE10

Suministrada por:

Alleima (formerly Sandvik Materials Technology)
Página 1 de 168