General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.85 g/cm³ Show Material materials with Densidad of 7.85 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Nickel Chromium Molybdenum Steel |
Elongación transversal | 20.0 °C | 12 % Show Material materials with Elongación transversal of 12 % | |
Límite elástico Rp 0,2 | 100.0 °C | 565 MPa Show Material materials with Límite elástico Rp 0,2 of 565 MPa | |
200.0 °C | 535 MPa Show Material materials with Límite elástico Rp 0,2 of 535 MPa | ||
250.0 °C | 515 MPa Show Material materials with Límite elástico Rp 0,2 of 515 MPa | ||
300.0 °C | 490 MPa Show Material materials with Límite elástico Rp 0,2 of 490 MPa | ||
350.0 °C | 435 MPa Show Material materials with Límite elástico Rp 0,2 of 435 MPa | ||
400.0 °C | 405 MPa Show Material materials with Límite elástico Rp 0,2 of 405 MPa | ||
450.0 °C | 375 MPa Show Material materials with Límite elástico Rp 0,2 of 375 MPa | ||
Límite elástico transversal Rp 0,2 | 20.0 °C | 600 MPa Show Material materials with Límite elástico transversal Rp 0,2 of 600 MPa | |
Módulo elástico | -100.0 °C | 217 GPa Show Material materials with Módulo elástico of 217 GPa | |
20.0 °C | 212 GPa Show Material materials with Módulo elástico of 212 GPa | ||
100.0 °C | 207 GPa Show Material materials with Módulo elástico of 207 GPa | ||
200.0 °C | 199 - 200 GPa Show Material materials with Módulo elástico of 199 - 200 GPa | ||
300.0 °C | 192 - 193 GPa Show Material materials with Módulo elástico of 192 - 193 GPa | ||
400.0 °C | 184 GPa Show Material materials with Módulo elástico of 184 GPa | ||
500.0 °C | 175 GPa Show Material materials with Módulo elástico of 175 GPa | ||
600.0 °C | 164 GPa Show Material materials with Módulo elástico of 164 GPa | ||
Reducción de área, transversal | 20.0 °C | 40 % Show Material materials with Reducción de área, transversal of 40 % | |
Resistencia a la tracción transversal | 20.0 °C | 750 - 900 MPa Show Material materials with Resistencia a la tracción transversal of 750 - 900 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | -100.0 °C | 423 J/(kg·K) Show Material materials with Calor específico of 423 J/(kg·K) | |
20.0 °C | 461 J/(kg·K) Show Material materials with Calor específico of 461 J/(kg·K) | ||
100.0 °C | 479 J/(kg·K) Show Material materials with Calor específico of 479 J/(kg·K) | ||
200.0 °C | 499 J/(kg·K) Show Material materials with Calor específico of 499 J/(kg·K) | ||
300.0 °C | 517 J/(kg·K) Show Material materials with Calor específico of 517 J/(kg·K) | ||
400.0 °C | 536 J/(kg·K) Show Material materials with Calor específico of 536 J/(kg·K) | ||
500.0 °C | 558 J/(kg·K) Show Material materials with Calor específico of 558 J/(kg·K) | ||
600.0 °C | 587 J/(kg·K) Show Material materials with Calor específico of 587 J/(kg·K) | ||
Coeficiente de dilatación térmica | -100.0 °C | 1.05E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.05E-5 1/K | |
20.0 °C | 1.15E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.15E-5 1/K | ||
100.0 °C | 1.11E-5 - 1.21E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.11E-5 - 1.21E-5 1/K | ||
200.0 °C | 1.21E-5 - 1.27E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.21E-5 - 1.27E-5 1/K | ||
300.0 °C | 1.29E-5 - 1.32E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.29E-5 - 1.32E-5 1/K | ||
400.0 °C | 1.35E-5 - 1.36E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.35E-5 - 1.36E-5 1/K | ||
500.0 °C | 1.39E-5 - 1.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.39E-5 - 1.4E-5 1/K | ||
600.0 °C | 1.41E-5 - 1.44E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.41E-5 - 1.44E-5 1/K | ||
Conductividad térmica | 20.0 °C | 47.1 W/(m·K) Show Material materials with Conductividad térmica of 47.1 W/(m·K) | |
100.0 °C | 43 - 47.1 W/(m·K) Show Material materials with Conductividad térmica of 43 - 47.1 W/(m·K) | ||
200.0 °C | 42 - 45.9 W/(m·K) Show Material materials with Conductividad térmica of 42 - 45.9 W/(m·K) | ||
300.0 °C | 40 - 43.8 W/(m·K) Show Material materials with Conductividad térmica of 40 - 43.8 W/(m·K) | ||
400.0 °C | 37 - 41.3 W/(m·K) Show Material materials with Conductividad térmica of 37 - 41.3 W/(m·K) | ||
500.0 °C | 34 - 38.7 W/(m·K) Show Material materials with Conductividad térmica of 34 - 38.7 W/(m·K) | ||
600.0 °C | 36 W/(m·K) Show Material materials with Conductividad térmica of 36 W/(m·K) | ||
Difusividad térmica | 20.0 °C | 13 mm²/s Show Material materials with Difusividad térmica of 13 mm²/s | |
100.0 °C | 12.1 mm²/s Show Material materials with Difusividad térmica of 12.1 mm²/s | ||
200.0 °C | 11.1 mm²/s Show Material materials with Difusividad térmica of 11.1 mm²/s | ||
300.0 °C | 9.9 mm²/s Show Material materials with Difusividad térmica of 9.9 mm²/s | ||
400.0 °C | 8.7 mm²/s Show Material materials with Difusividad térmica of 8.7 mm²/s | ||
500.0 °C | 7.4 mm²/s Show Material materials with Difusividad térmica of 7.4 mm²/s | ||
600.0 °C | 6 mm²/s Show Material materials with Difusividad térmica of 6 mm²/s | ||
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Nickel Chromium Molybdenum Steel | |
Temperatura máx. de funcionamiento, largo | 370 - 480 °C Show Material materials with Temperatura máx. de funcionamiento, largo of 370 - 480 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 2.21E-7 Ω·m Show Material materials with Resistividad eléctrica of 2.21E-7 Ω·m |
100.0 °C | 2.72E-7 Ω·m Show Material materials with Resistividad eléctrica of 2.72E-7 Ω·m | |
200.0 °C | 3.44E-7 Ω·m Show Material materials with Resistividad eléctrica of 3.44E-7 Ω·m | |
300.0 °C | 4.28E-7 Ω·m Show Material materials with Resistividad eléctrica of 4.28E-7 Ω·m | |
400.0 °C | 5.26E-7 Ω·m Show Material materials with Resistividad eléctrica of 5.26E-7 Ω·m | |
500.0 °C | 6.39E-7 Ω·m Show Material materials with Resistividad eléctrica of 6.39E-7 Ω·m | |
600.0 °C | 7.7E-7 Ω·m Show Material materials with Resistividad eléctrica of 7.7E-7 Ω·m | |
Chemical properties
Property | Value |
---|---|
Azufre | 0.007 - 0.018 % Show Material materials with Azufre of 0.007 - 0.018 % |
Carbono | 0.2 - 0.26 % Show Material materials with Carbono of 0.2 - 0.26 % |
Cromo | 1.7 - 2 % Show Material materials with Cromo of 1.7 - 2 % |
Fósforo | 0.01 - 0.02 % Show Material materials with Fósforo of 0.01 - 0.02 % |
Manganeso | 0.5 - 0.8 % Show Material materials with Manganeso of 0.5 - 0.8 % |
Molibdeno | 0.6 - 0.8 % Show Material materials with Molibdeno of 0.6 - 0.8 % |
Níquel | 0.9 - 1.2 % Show Material materials with Níquel of 0.9 - 1.2 % |
Silicona | 0.3 % Show Material materials with Silicona of 0.3 % |