Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00Wrought Copper High Copper Alloy
ASTM B194 Grade C17200 TD04Wrought Copper High Copper Alloy
ASTM B768 Grade C17510 TH04Wrought Copper High Copper Alloy
EN 1652 Grade C17200 TF00Chromium Molybdenum Steel
DIN 17175 Grade 14MoV6-3 quenched and tempered (+QT)Nickel Chromium Molybdenum Steel
EN 10083-1 Grade 30CrNiMo8 quenched and tempered (+QT)Nickel Chromium Molybdenum Steel
EN 10083-1 Grade 34CrNiMo6 quenched and tempered (+QT)Chromium Molybdenum Steel
EN 10222-2 Grade 14MoV6-3 normalized and tempered (+NT)Nickel Chromium Molybdenum Steel
SEW 555 Grade 23CrNiMo7-4-7 quenched and tempered (+QT)Nickel Chromium Molybdenum Steel
EN 10277-5 Grade 34CrNiMo6 quenched and tempered and cold drawn (+QT+C)Nickel Chromium Molybdenum Steel
EN 10277-5 Grade 34CrNiMo6 cold drawn and quenched and tempered (+C+QT)Nickel Chromium Steel
SEW 555 Grade 30CrMoNiV5-11 quenched and tempered (+QT)Nickel Chromium Steel
SEW 555 Grade 28CrMoNiV4-9 quenched and tempered (+QT)Nickel Chromium Molybdenum Steel
EN 10263-3 Grade 21NiCrMo2 annealed to achieve spheroidized carbides (+AC)Nickel Chromium Molybdenum Steel
EN 10263-3 Grade 21NiCrMo2 annealed to achieve spheroidized carbides and turnedNickel Chromium Molybdenum Steel
EN 10263-3 Grade 21NiCrMo2 cold drawn, annealed to achieve spheroidized carbides and slightly skin passedNitriding Steel
EN 10085 Grade 31CrMoV9 quenched and tempered (+QT)Nickel Chromium Molybdenum Steel
DIN 1652-3 Grade 21NiCrMo2 treated to ferritic-pearlite structure and cold-drawnNickel Chromium Molybdenum Steel
DIN 1652-3 Grade 21NiCrMo2 cold drawnNickel Chromium Molybdenum Steel
DIN 1652-3 Grade 21NiCrMo2 cold-drawn or peeled and treated to ferrite-pearlite structure