General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Low Carbon Steel | ||||
Dureza Brinell | 241 [-] Show Material materials with Dureza Brinell of 241 [-] | Predicted Value, Transverse | ||||
Elongación | 18.3 % Show Material materials with Elongación of 18.3 % | Predicted Value, A200 | ||||
21.0 % Show Material materials with Elongación of 21.0 % | Predicted Value, A80 Transverse | |||||
21.3 % Show Material materials with Elongación of 21.3 % | Predicted Value, A5 | |||||
22.2 % Show Material materials with Elongación of 22.2 % | Predicted Value, A50 | |||||
23.1 % Show Material materials with Elongación of 23.1 % | Predicted Value, Transverse | |||||
20 °C | 20 % Show Material materials with Elongación of 20 % | thermomechanically rolled | EN 10149-2 | Flat | A80 | |
20 °C | 24 % Show Material materials with Elongación of 24 % | thermomechanically rolled | EN 10149-2 | Flat | ||
Estricción | 40.6 % Show Material materials with Estricción of 40.6 % | Predicted Value | ||||
44.4 % Show Material materials with Estricción of 44.4 % | Predicted Value, Transverse | |||||
Límite elástico | 251.8 MPa Show Material materials with Límite elástico of 251.8 MPa | Predicted Value, RP1 | ||||
315.4 MPa Show Material materials with Límite elástico of 315.4 MPa | Predicted Value, RP1 Transverse | |||||
332.9 MPa Show Material materials with Límite elástico of 332.9 MPa | Predicted Value, RP02 | |||||
345.1 MPa Show Material materials with Límite elástico of 345.1 MPa | Predicted Value, Transverse | |||||
405.9 MPa Show Material materials with Límite elástico of 405.9 MPa | Predicted Value, RP05 | |||||
483.3 MPa Show Material materials with Límite elástico of 483.3 MPa | Predicted Value, RP02 Transverse | |||||
488 MPa Show Material materials with Límite elástico of 488 MPa | Predicted Value, RP002 | |||||
20 °C | 315 MPa Show Material materials with Límite elástico of 315 MPa | thermomechanically rolled | EN 10149-2 | Flat | ||
Módulo de cizallamiento | 82 GPa Show Material materials with Módulo de cizallamiento of 82 GPa | Typical for Low Carbon Steel | ||||
Módulo elástico | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Low Carbon Steel | ||||
Resistencia a la tracción | 20 °C | 390 - 510 MPa Show Material materials with Resistencia a la tracción of 390 - 510 MPa | thermomechanically rolled | EN 10149-2 | Flat | |
Resistencia al cizallamiento | 532.2 MPa Show Material materials with Resistencia al cizallamiento of 532.2 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Calor específico | 465 J/(kg·K) Show Material materials with Calor específico of 465 J/(kg·K) | Typical for Low Carbon Steel | |||
Coeficiente de dilatación térmica | 1.32e-05 - 1.38e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.32e-05 - 1.38e-05 1/K | Typical for Low Carbon Steel | |||
Conductividad térmica | 25 - 93 W/(m·K) Show Material materials with Conductividad térmica of 25 - 93 W/(m·K) | Typical for Low Carbon Steel | |||
Temperatura de fusión | 1480 - 1526 °C Show Material materials with Temperatura de fusión of 1480 - 1526 °C | Typical for Low Carbon Steel | |||
Temperatura máx. de funcionamiento | -20 °C Show Material materials with Temperatura máx. de funcionamiento of -20 °C | thermomechanically rolled | EN 10149-2 | Flat | Long |
500 °C Show Material materials with Temperatura máx. de funcionamiento of 500 °C | Typical for Carbon Steel |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 7 S/m Show Material materials with Conductividad eléctrica of 7 S/m | Predicted Value |
Resistividad eléctrica | 1.43e-07 - 1.74e-07 Ω·m Show Material materials with Resistividad eléctrica of 1.43e-07 - 1.74e-07 Ω·m | Typical for Carbon Steel |
Magnético
Property | Value | Comment |
---|---|---|
Temperatura de Curie | 770 °C Show Material materials with Temperatura de Curie of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 0.015 % Show Material materials with Aluminio of 0.015 % | thermomechanically rolled | EN 10149-2 | Flat |
Azufre | 0.02 % Show Material materials with Azufre of 0.02 % | thermomechanically rolled | EN 10149-2 | Flat |
Carbono | 0.12 % Show Material materials with Carbono of 0.12 % | thermomechanically rolled | EN 10149-2 | Flat |
Fósforo | 0.025 % Show Material materials with Fósforo of 0.025 % | thermomechanically rolled | EN 10149-2 | Flat |
Manganeso | 1.3 % Show Material materials with Manganeso of 1.3 % | thermomechanically rolled | EN 10149-2 | Flat |
Niobio | 0.09 % Show Material materials with Niobio of 0.09 % | thermomechanically rolled | EN 10149-2 | Flat |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % | thermomechanically rolled | EN 10149-2 | Flat |
Titanio | 0.15 % Show Material materials with Titanio of 0.15 % | thermomechanically rolled | EN 10149-2 | Flat |
Vanadio | 0.2 % Show Material materials with Vanadio of 0.2 % | thermomechanically rolled | EN 10149-2 | Flat |