General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel | ||||
Dureza Brinell | 249 [-] Show Material materials with Dureza Brinell of 249 [-] | Predicted Value, Transverse | ||||
Elongación | 13.2 % Show Material materials with Elongación of 13.2 % | Predicted Value, A200 | ||||
13.3 % Show Material materials with Elongación of 13.3 % | Predicted Value, Transverse | |||||
17.7 % Show Material materials with Elongación of 17.7 % | Predicted Value, A80 Transverse | |||||
18.6 % Show Material materials with Elongación of 18.6 % | Predicted Value, A5 | |||||
18.6 % Show Material materials with Elongación of 18.6 % | Predicted Value, A50 | |||||
20 °C | 11 % Show Material materials with Elongación of 11 % | thermomechanically rolled | EN 10149-2 | Flat | A80 | |
20 °C | 11 % Show Material materials with Elongación of 11 % | thermomechanically rolled | EN 10149-2 | Flat | ||
20 °C | 13 % Show Material materials with Elongación of 13 % | thermomechanically rolled | EN 10149-2 | Flat | A80 | |
20 °C | 13 % Show Material materials with Elongación of 13 % | thermomechanically rolled | EN 10149-2 | Flat | ||
Estricción | 39.6 % Show Material materials with Estricción of 39.6 % | Predicted Value | ||||
44.2 % Show Material materials with Estricción of 44.2 % | Predicted Value, Transverse | |||||
Límite elástico | 288.4 MPa Show Material materials with Límite elástico of 288.4 MPa | Predicted Value, RP1 | ||||
328.2 MPa Show Material materials with Límite elástico of 328.2 MPa | Predicted Value, RP1 Transverse | |||||
493.8 MPa Show Material materials with Límite elástico of 493.8 MPa | Predicted Value, Transverse | |||||
501.6 MPa Show Material materials with Límite elástico of 501.6 MPa | Predicted Value, RP02 Transverse | |||||
524.2 MPa Show Material materials with Límite elástico of 524.2 MPa | Predicted Value, RP02 | |||||
547.5 MPa Show Material materials with Límite elástico of 547.5 MPa | Predicted Value, RP05 | |||||
619.8 MPa Show Material materials with Límite elástico of 619.8 MPa | Predicted Value, RP002 | |||||
20 °C | 600 MPa Show Material materials with Límite elástico of 600 MPa | thermomechanically rolled | EN 10149-2 | Flat | ||
Módulo de cizallamiento | 80.2 GPa Show Material materials with Módulo de cizallamiento of 80.2 GPa | Predicted Value | ||||
Módulo elástico | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel | ||||
Resistencia a la tracción | 20 °C | 650 - 820 MPa Show Material materials with Resistencia a la tracción of 650 - 820 MPa | thermomechanically rolled | EN 10149-2 | Flat | |
Resistencia al cizallamiento | 571.7 MPa Show Material materials with Resistencia al cizallamiento of 571.7 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 453.5 J/(kg·K) Show Material materials with Calor específico of 453.5 J/(kg·K) | Predicted Value |
Coeficiente de dilatación térmica | 11.98 1/K Show Material materials with Coeficiente de dilatación térmica of 11.98 1/K | Predicted Value |
Conductividad térmica | 37.81 W/(m·K) Show Material materials with Conductividad térmica of 37.81 W/(m·K) | Predicted Value |
Eléctrico
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 0.015 % Show Material materials with Aluminio of 0.015 % | thermomechanically rolled | EN 10149-2 | Flat |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % | thermomechanically rolled | EN 10149-2 | Flat |
Boro | 0.005 % Show Material materials with Boro of 0.005 % | thermomechanically rolled | EN 10149-2 | Flat |
Carbono | 0.12 % Show Material materials with Carbono of 0.12 % | thermomechanically rolled | EN 10149-2 | Flat |
Fósforo | 0.025 % Show Material materials with Fósforo of 0.025 % | thermomechanically rolled | EN 10149-2 | Flat |
Manganeso | 1.9 % Show Material materials with Manganeso of 1.9 % | thermomechanically rolled | EN 10149-2 | Flat |
Molibdeno | 0.5 % Show Material materials with Molibdeno of 0.5 % | thermomechanically rolled | EN 10149-2 | Flat |
Niobio | 0.09 % Show Material materials with Niobio of 0.09 % | thermomechanically rolled | EN 10149-2 | Flat |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % | thermomechanically rolled | EN 10149-2 | Flat |
Titanio | 0.22 % Show Material materials with Titanio of 0.22 % | thermomechanically rolled | EN 10149-2 | Flat |
Vanadio | 0.2 % Show Material materials with Vanadio of 0.2 % | thermomechanically rolled | EN 10149-2 | Flat |