General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel | ||||
Dureza Brinell | 248 [-] Show Material materials with Dureza Brinell of 248 [-] | Predicted Value, Transverse | ||||
Elongación | 13.0 % Show Material materials with Elongación of 13.0 % | Predicted Value, A200 | ||||
13.2 % Show Material materials with Elongación of 13.2 % | Predicted Value, Transverse | |||||
17.5 % Show Material materials with Elongación of 17.5 % | Predicted Value, A50 | |||||
17.5 % Show Material materials with Elongación of 17.5 % | Predicted Value, A80 Transverse | |||||
18.3 % Show Material materials with Elongación of 18.3 % | Predicted Value, A5 | |||||
20 °C | 10 % Show Material materials with Elongación of 10 % | thermomechanically rolled | EN 10149-2 | Flat | A80 | |
20 °C | 10 % Show Material materials with Elongación of 10 % | thermomechanically rolled | EN 10149-2 | Flat | ||
20 °C | 12 % Show Material materials with Elongación of 12 % | thermomechanically rolled | EN 10149-2 | Flat | A80 | |
20 °C | 12 % Show Material materials with Elongación of 12 % | thermomechanically rolled | EN 10149-2 | Flat | ||
Estricción | 38.9 % Show Material materials with Estricción of 38.9 % | Predicted Value | ||||
44.1 % Show Material materials with Estricción of 44.1 % | Predicted Value, Transverse | |||||
Límite elástico | 293.5 MPa Show Material materials with Límite elástico of 293.5 MPa | Predicted Value, RP1 | ||||
328.8 MPa Show Material materials with Límite elástico of 328.8 MPa | Predicted Value, RP1 Transverse | |||||
505.4 MPa Show Material materials with Límite elástico of 505.4 MPa | Predicted Value, RP02 Transverse | |||||
525.6 MPa Show Material materials with Límite elástico of 525.6 MPa | Predicted Value, Transverse | |||||
547.5 MPa Show Material materials with Límite elástico of 547.5 MPa | Predicted Value, RP05 | |||||
562.8 MPa Show Material materials with Límite elástico of 562.8 MPa | Predicted Value, RP02 | |||||
623.6 MPa Show Material materials with Límite elástico of 623.6 MPa | Predicted Value, RP002 | |||||
20 °C | 650 MPa Show Material materials with Límite elástico of 650 MPa | thermomechanically rolled | EN 10149-2 | Flat | ||
Módulo de cizallamiento | 80.1 GPa Show Material materials with Módulo de cizallamiento of 80.1 GPa | Predicted Value | ||||
Módulo elástico | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel | ||||
Resistencia a la tracción | 20 °C | 700 - 880 MPa Show Material materials with Resistencia a la tracción of 700 - 880 MPa | thermomechanically rolled | EN 10149-2 | Flat | |
Resistencia al cizallamiento | 583.8 MPa Show Material materials with Resistencia al cizallamiento of 583.8 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 453.9 J/(kg·K) Show Material materials with Calor específico of 453.9 J/(kg·K) | Predicted Value |
Coeficiente de dilatación térmica | 11.96 1/K Show Material materials with Coeficiente de dilatación térmica of 11.96 1/K | Predicted Value |
Conductividad térmica | 37.64 W/(m·K) Show Material materials with Conductividad térmica of 37.64 W/(m·K) | Predicted Value |
Eléctrico
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 0.015 % Show Material materials with Aluminio of 0.015 % | thermomechanically rolled | EN 10149-2 | Flat |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % | thermomechanically rolled | EN 10149-2 | Flat |
Boro | 0.005 % Show Material materials with Boro of 0.005 % | thermomechanically rolled | EN 10149-2 | Flat |
Carbono | 0.12 % Show Material materials with Carbono of 0.12 % | thermomechanically rolled | EN 10149-2 | Flat |
Fósforo | 0.025 % Show Material materials with Fósforo of 0.025 % | thermomechanically rolled | EN 10149-2 | Flat |
Manganeso | 2 % Show Material materials with Manganeso of 2 % | thermomechanically rolled | EN 10149-2 | Flat |
Molibdeno | 0.5 % Show Material materials with Molibdeno of 0.5 % | thermomechanically rolled | EN 10149-2 | Flat |
Niobio | 0.09 % Show Material materials with Niobio of 0.09 % | thermomechanically rolled | EN 10149-2 | Flat |
Silicona | 0.6 % Show Material materials with Silicona of 0.6 % | thermomechanically rolled | EN 10149-2 | Flat |
Titanio | 0.22 % Show Material materials with Titanio of 0.22 % | thermomechanically rolled | EN 10149-2 | Flat |
Vanadio | 0.2 % Show Material materials with Vanadio of 0.2 % | thermomechanically rolled | EN 10149-2 | Flat |