General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Medium Carbon Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Medium Carbon Steel |
Dureza Brinell | 23.0 °C | 197 [-] Show Material materials with Dureza Brinell of 197 [-] | Soft Annealed |
Dureza Vickers | 23.0 °C | 510 [-] Show Material materials with Dureza Vickers of 510 [-] | Hardened |
Elongación | 23.0 °C | 16 % Show Material materials with Elongación of 16 % | |
Límite elástico | 23.0 °C | 260 - 320 MPa Show Material materials with Límite elástico of 260 - 320 MPa | |
Módulo de cizallamiento | 23.0 °C | 75 - 80 GPa Show Material materials with Módulo de cizallamiento of 75 - 80 GPa | Typical for Carbon Steel |
Módulo elástico | 23.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Medium Carbon Steel |
Resistencia a la tracción | 23.0 °C | 530 - 580 MPa Show Material materials with Resistencia a la tracción of 530 - 580 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 470 - 520 J/(kg·K) Show Material materials with Calor específico of 470 - 520 J/(kg·K) | Typical for Medium Carbon Steel |
Coeficiente de dilatación térmica | 23.0 °C | 1.32E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.32E-5 1/K | Typical for Medium Carbon Steel |
Conductividad térmica | 23.0 °C | 21 - 52 W/(m·K) Show Material materials with Conductividad térmica of 21 - 52 W/(m·K) | Typical for Medium Carbon Steel |
Temperatura de fusión | 1380 - 1514 °C Show Material materials with Temperatura de fusión of 1380 - 1514 °C | Typical for Medium Carbon Steel | |
Temperatura máx. de funcionamiento | 500 °C Show Material materials with Temperatura máx. de funcionamiento of 500 °C | Typical for Carbon Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with Resistividad eléctrica of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.045 % Show Material materials with Azufre of 0.045 % |
Carbono | 0.37 - 0.44 % Show Material materials with Carbono of 0.37 - 0.44 % |
Cromo | 0.4 % Show Material materials with Cromo of 0.4 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Manganeso | 0.5 - 0.8 % Show Material materials with Manganeso of 0.5 - 0.8 % |
Molibdeno | 0.1 % Show Material materials with Molibdeno of 0.1 % |
Níquel | 0.4 % Show Material materials with Níquel of 0.4 % |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % |