General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Low Carbon Steel | ||||
Dureza Brinell | 239 [-] Show Material materials with Dureza Brinell of 239 [-] | Predicted Value, Transverse | ||||
Elongación | 18.2 % Show Material materials with Elongación of 18.2 % | Predicted Value, A200 | ||||
19.7 % Show Material materials with Elongación of 19.7 % | Predicted Value, A5 | |||||
20.4 % Show Material materials with Elongación of 20.4 % | Predicted Value, A80 Transverse | |||||
23.7 % Show Material materials with Elongación of 23.7 % | Predicted Value, Transverse | |||||
24.8 % Show Material materials with Elongación of 24.8 % | Predicted Value, A50 | |||||
20 °C | 19 % Show Material materials with Elongación of 19 % | normalized or normalized formed (+N) | EN 10207 | Strip, Sheet, Bar | A80 | |
20 °C | 20 % Show Material materials with Elongación of 20 % | normalized or normalized formed (+N) | EN 10207 | Strip, Sheet, Bar | A80 | |
20 °C | 24 % Show Material materials with Elongación of 24 % | normalized or normalized formed (+N) | EN 10207 | Strip, Sheet, Bar | ||
Estricción | 42.4 % Show Material materials with Estricción of 42.4 % | Predicted Value, Transverse | ||||
43.2 % Show Material materials with Estricción of 43.2 % | Predicted Value | |||||
Límite elástico | 259.3 MPa Show Material materials with Límite elástico of 259.3 MPa | Predicted Value, RP1 | ||||
314.8 MPa Show Material materials with Límite elástico of 314.8 MPa | Predicted Value, Transverse | |||||
316.9 MPa Show Material materials with Límite elástico of 316.9 MPa | Predicted Value, RP05 | |||||
337.4 MPa Show Material materials with Límite elástico of 337.4 MPa | Predicted Value, RP1 Transverse | |||||
451.8 MPa Show Material materials with Límite elástico of 451.8 MPa | Predicted Value, RP002 | |||||
470.5 MPa Show Material materials with Límite elástico of 470.5 MPa | Predicted Value, RP02 Transverse | |||||
20 °C | 255 MPa Show Material materials with Límite elástico of 255 MPa | normalized or normalized formed (+N) | EN 10207 | Strip, Sheet, Bar | ||
20 °C | 265 MPa Show Material materials with Límite elástico of 265 MPa | normalized or normalized formed (+N) | EN 10207 | Strip, Sheet, Bar | ||
20 °C | 275 MPa Show Material materials with Límite elástico of 275 MPa | normalized or normalized formed (+N) | EN 10207 | Strip, Sheet, Bar | ||
100 °C | 212 MPa Show Material materials with Límite elástico of 212 MPa | normalized or normalized formed (+N) | EN 10207 | Strip, Sheet, Bar | RP02 | |
100 °C | 221 MPa Show Material materials with Límite elástico of 221 MPa | normalized or normalized formed (+N) | EN 10207 | Strip, Sheet, Bar | RP02 | |
150 °C | 194 MPa Show Material materials with Límite elástico of 194 MPa | normalized or normalized formed (+N) | EN 10207 | Strip, Sheet, Bar | RP02 | |
150 °C | 203 MPa Show Material materials with Límite elástico of 203 MPa | normalized or normalized formed (+N) | EN 10207 | Strip, Sheet, Bar | RP02 | |
200 °C | 176 MPa Show Material materials with Límite elástico of 176 MPa | normalized or normalized formed (+N) | EN 10207 | Strip, Sheet, Bar | RP02 | |
250 °C | 159 MPa Show Material materials with Límite elástico of 159 MPa | normalized or normalized formed (+N) | EN 10207 | Strip, Sheet, Bar | RP02 | |
300 °C | 132 MPa Show Material materials with Límite elástico of 132 MPa | normalized or normalized formed (+N) | EN 10207 | Strip, Sheet, Bar | RP02 | |
Módulo de cizallamiento | 82 GPa Show Material materials with Módulo de cizallamiento of 82 GPa | Typical for Low Carbon Steel | ||||
Módulo elástico | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Low Carbon Steel | ||||
Resistencia a la tracción | 20 °C | 390 - 510 MPa Show Material materials with Resistencia a la tracción of 390 - 510 MPa | normalized or normalized formed (+N) | EN 10207 | Strip, Sheet, Bar | |
Resistencia al cizallamiento | 519.3 MPa Show Material materials with Resistencia al cizallamiento of 519.3 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 465 J/(kg·K) Show Material materials with Calor específico of 465 J/(kg·K) | Typical for Low Carbon Steel |
Coeficiente de dilatación térmica | 1.32e-05 - 1.38e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.32e-05 - 1.38e-05 1/K | Typical for Low Carbon Steel |
Conductividad térmica | 25 - 93 W/(m·K) Show Material materials with Conductividad térmica of 25 - 93 W/(m·K) | Typical for Low Carbon Steel |
Temperatura de fusión | 1480 - 1526 °C Show Material materials with Temperatura de fusión of 1480 - 1526 °C | Typical for Low Carbon Steel |
Temperatura máx. de funcionamiento | 303.3 °C Show Material materials with Temperatura máx. de funcionamiento of 303.3 °C | Predicted Value, Long |
500 °C Show Material materials with Temperatura máx. de funcionamiento of 500 °C | Typical for Carbon Steel |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 7 S/m Show Material materials with Conductividad eléctrica of 7 S/m | Predicted Value |
Resistividad eléctrica | 1.43e-07 - 1.74e-07 Ω·m Show Material materials with Resistividad eléctrica of 1.43e-07 - 1.74e-07 Ω·m | Typical for Carbon Steel |
Magnético
Property | Value | Comment |
---|---|---|
Temperatura de Curie | 770 °C Show Material materials with Temperatura de Curie of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 0.02 % Show Material materials with Aluminio of 0.02 % | normalized or normalized formed (+N) | EN 10207 | Strip, Sheet, Bar |
Azufre | 0.02 % Show Material materials with Azufre of 0.02 % | normalized or normalized formed (+N) | EN 10207 | Strip, Sheet, Bar |
Carbono | 0.16 % Show Material materials with Carbono of 0.16 % | normalized or normalized formed (+N) | EN 10207 | Strip, Sheet, Bar |
Fósforo | 0.025 % Show Material materials with Fósforo of 0.025 % | normalized or normalized formed (+N) | EN 10207 | Strip, Sheet, Bar |
Manganeso | 0.5 - 1.5 % Show Material materials with Manganeso of 0.5 - 1.5 % | normalized or normalized formed (+N) | EN 10207 | Strip, Sheet, Bar |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % | normalized or normalized formed (+N) | EN 10207 | Strip, Sheet, Bar |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |