General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.7 g/cm³ Show Material materials with Densidad of 7.7 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.28 [-] Show Material materials with Coeficiente de Poisson of 0.28 [-] |
95.0 °C | 0.27 [-] Show Material materials with Coeficiente de Poisson of 0.27 [-] | |
150.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | |
205.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | |
260.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | |
315.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | |
370.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | |
425.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | |
Dureza Brinell | 20.0 °C | 212 [-] Show Material materials with Dureza Brinell of 212 [-] |
Elongación | 20.0 °C | 15 % Show Material materials with Elongación of 15 % |
Elongación A80 | 20.0 °C | 13 % Show Material materials with Elongación A80 of 13 % |
Límite elástico Rp 0,2 | 20.0 °C | 280 MPa Show Material materials with Límite elástico Rp 0,2 of 280 MPa |
Módulo de cizallamiento | 20.0 °C | 82.05 GPa Show Material materials with Módulo de cizallamiento of 82.05 GPa |
95.0 °C | 80.67 GPa Show Material materials with Módulo de cizallamiento of 80.67 GPa | |
150.0 °C | 78.6 GPa Show Material materials with Módulo de cizallamiento of 78.6 GPa | |
205.0 °C | 77.22 GPa Show Material materials with Módulo de cizallamiento of 77.22 GPa | |
260.0 °C | 75.15 GPa Show Material materials with Módulo de cizallamiento of 75.15 GPa | |
315.0 °C | 73.77 GPa Show Material materials with Módulo de cizallamiento of 73.77 GPa | |
370.0 °C | 71.71 GPa Show Material materials with Módulo de cizallamiento of 71.71 GPa | |
425.0 °C | 68.95 GPa Show Material materials with Módulo de cizallamiento of 68.95 GPa | |
Módulo elástico | 20.0 °C | 209.6 GPa Show Material materials with Módulo elástico of 209.6 GPa |
95.0 °C | 205.46 GPa Show Material materials with Módulo elástico of 205.46 GPa | |
150.0 °C | 202.71 GPa Show Material materials with Módulo elástico of 202.71 GPa | |
205.0 °C | 198.57 GPa Show Material materials with Módulo elástico of 198.57 GPa | |
260.0 °C | 195.12 GPa Show Material materials with Módulo elástico of 195.12 GPa | |
315.0 °C | 190.99 GPa Show Material materials with Módulo elástico of 190.99 GPa | |
370.0 °C | 185.47 GPa Show Material materials with Módulo elástico of 185.47 GPa | |
425.0 °C | 179.26 GPa Show Material materials with Módulo elástico of 179.26 GPa | |
Resistencia a la tracción | 20.0 °C | 500 - 700 MPa Show Material materials with Resistencia a la tracción of 500 - 700 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 500 J/(kg·K) Show Material materials with Calor específico of 500 J/(kg·K) | |
Coeficiente de dilatación térmica | 200.0 °C | 1E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1E-5 1/K | |
400.0 °C | 1.1E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.1E-5 1/K | ||
600.0 °C | 1.15E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.15E-5 1/K | ||
800.0 °C | 1.2E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.2E-5 1/K | ||
1000.0 °C | 1.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.3E-5 1/K | ||
Conductividad térmica | 20.0 °C | 17 W/(m·K) Show Material materials with Conductividad térmica of 17 W/(m·K) | |
500.0 °C | 23 W/(m·K) Show Material materials with Conductividad térmica of 23 W/(m·K) | ||
Temperatura de fusión | 1425 - 1530 °C Show Material materials with Temperatura de fusión of 1425 - 1530 °C | Typical for Ferritic Stainless Steel | |
Temperatura máx. de funcionamiento, largo | 0 - 1000 °C Show Material materials with Temperatura máx. de funcionamiento, largo of 0 - 1000 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 7E-7 Ω·m Show Material materials with Resistividad eléctrica of 7E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.15 - 0.2 % Show Material materials with Carbono of 0.15 - 0.2 % |
Cromo | 26 - 29 % Show Material materials with Cromo of 26 - 29 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Nitrógeno | 0.15 - 0.25 % Show Material materials with Nitrógeno of 0.15 - 0.25 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |