General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.98 - 8 g/cm³ Show Material materials with Densidad of 7.98 - 8 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Brinell | 20.0 °C | 223 [-] Show Material materials with Dureza Brinell of 223 [-] | |
Elongación | 20.0 °C | 30 % Show Material materials with Elongación of 30 % | |
Elongación A80 | 20.0 °C | 28 % Show Material materials with Elongación A80 of 28 % | |
Límite elástico Rp 0,2 | 20.0 °C | 230 MPa Show Material materials with Límite elástico Rp 0,2 of 230 MPa | |
Límite elástico Rp 1,0 | 20.0 °C | 270 MPa Show Material materials with Límite elástico Rp 1,0 of 270 MPa | |
Módulo elástico | -100.0 °C | 201 GPa Show Material materials with Módulo elástico of 201 GPa | |
20.0 °C | 194 GPa Show Material materials with Módulo elástico of 194 GPa | ||
100.0 °C | 189 GPa Show Material materials with Módulo elástico of 189 GPa | ||
200.0 °C | 183 GPa Show Material materials with Módulo elástico of 183 GPa | ||
300.0 °C | 177 GPa Show Material materials with Módulo elástico of 177 GPa | ||
400.0 °C | 170 GPa Show Material materials with Módulo elástico of 170 GPa | ||
500.0 °C | 163 GPa Show Material materials with Módulo elástico of 163 GPa | ||
600.0 °C | 156 GPa Show Material materials with Módulo elástico of 156 GPa | ||
700.0 °C | 149 GPa Show Material materials with Módulo elástico of 149 GPa | ||
800.0 °C | 141 GPa Show Material materials with Módulo elástico of 141 GPa | ||
900.0 °C | 134 GPa Show Material materials with Módulo elástico of 134 GPa | ||
1000.0 °C | 127 GPa Show Material materials with Módulo elástico of 127 GPa | ||
Resistencia a la tracción | 20.0 °C | 550 - 750 MPa Show Material materials with Resistencia a la tracción of 550 - 750 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | -100.0 °C | 440 J/(kg·K) Show Material materials with Calor específico of 440 J/(kg·K) |
20.0 °C | 472 - 550 J/(kg·K) Show Material materials with Calor específico of 472 - 550 J/(kg·K) | |
100.0 °C | 487 J/(kg·K) Show Material materials with Calor específico of 487 J/(kg·K) | |
200.0 °C | 503 J/(kg·K) Show Material materials with Calor específico of 503 J/(kg·K) | |
300.0 °C | 512 J/(kg·K) Show Material materials with Calor específico of 512 J/(kg·K) | |
400.0 °C | 520 J/(kg·K) Show Material materials with Calor específico of 520 J/(kg·K) | |
500.0 °C | 530 J/(kg·K) Show Material materials with Calor específico of 530 J/(kg·K) | |
600.0 °C | 541 J/(kg·K) Show Material materials with Calor específico of 541 J/(kg·K) | |
700.0 °C | 551 J/(kg·K) Show Material materials with Calor específico of 551 J/(kg·K) | |
800.0 °C | 559 J/(kg·K) Show Material materials with Calor específico of 559 J/(kg·K) | |
900.0 °C | 565 J/(kg·K) Show Material materials with Calor específico of 565 J/(kg·K) | |
1000.0 °C | 571 J/(kg·K) Show Material materials with Calor específico of 571 J/(kg·K) | |
Coeficiente de dilatación térmica | -100.0 °C | 1.36E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.36E-5 1/K |
20.0 °C | 1.46E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.46E-5 1/K | |
100.0 °C | 1.51E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.51E-5 1/K | |
200.0 °C | 1.5E-5 - 1.57E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.5E-5 - 1.57E-5 1/K | |
300.0 °C | 1.62E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.62E-5 1/K | |
400.0 °C | 1.6E-5 - 1.66E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.66E-5 1/K | |
500.0 °C | 1.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 1/K | |
600.0 °C | 1.7E-5 - 1.74E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 - 1.74E-5 1/K | |
700.0 °C | 1.77E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.77E-5 1/K | |
800.0 °C | 1.75E-5 - 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.75E-5 - 1.8E-5 1/K | |
900.0 °C | 1.83E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.83E-5 1/K | |
1000.0 °C | 1.85E-5 - 1.86E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.85E-5 - 1.86E-5 1/K | |
Conductividad térmica | 20.0 °C | 11.4 - 12.5 W/(m·K) Show Material materials with Conductividad térmica of 11.4 - 12.5 W/(m·K) |
100.0 °C | 12.8 W/(m·K) Show Material materials with Conductividad térmica of 12.8 W/(m·K) | |
200.0 °C | 14.6 W/(m·K) Show Material materials with Conductividad térmica of 14.6 W/(m·K) | |
300.0 °C | 16.3 W/(m·K) Show Material materials with Conductividad térmica of 16.3 W/(m·K) | |
400.0 °C | 17.9 W/(m·K) Show Material materials with Conductividad térmica of 17.9 W/(m·K) | |
500.0 °C | 17 - 19.5 W/(m·K) Show Material materials with Conductividad térmica of 17 - 19.5 W/(m·K) | |
600.0 °C | 21 W/(m·K) Show Material materials with Conductividad térmica of 21 W/(m·K) | |
700.0 °C | 22.6 W/(m·K) Show Material materials with Conductividad térmica of 22.6 W/(m·K) | |
800.0 °C | 24.1 W/(m·K) Show Material materials with Conductividad térmica of 24.1 W/(m·K) | |
900.0 °C | 25.6 W/(m·K) Show Material materials with Conductividad térmica of 25.6 W/(m·K) | |
1000.0 °C | 27 W/(m·K) Show Material materials with Conductividad térmica of 27 W/(m·K) | |
Difusividad térmica | 20.0 °C | 3 mm²/s Show Material materials with Difusividad térmica of 3 mm²/s |
100.0 °C | 3.2 mm²/s Show Material materials with Difusividad térmica of 3.2 mm²/s | |
200.0 °C | 3.5 mm²/s Show Material materials with Difusividad térmica of 3.5 mm²/s | |
300.0 °C | 4 mm²/s Show Material materials with Difusividad térmica of 4 mm²/s | |
400.0 °C | 4.1 mm²/s Show Material materials with Difusividad térmica of 4.1 mm²/s | |
500.0 °C | 4.3 mm²/s Show Material materials with Difusividad térmica of 4.3 mm²/s | |
600.0 °C | 4.5 mm²/s Show Material materials with Difusividad térmica of 4.5 mm²/s | |
700.0 °C | 4.8 mm²/s Show Material materials with Difusividad térmica of 4.8 mm²/s | |
800.0 °C | 5.2 mm²/s Show Material materials with Difusividad térmica of 5.2 mm²/s | |
900.0 °C | 5.5 mm²/s Show Material materials with Difusividad térmica of 5.5 mm²/s | |
1000.0 °C | 5.6 mm²/s Show Material materials with Difusividad térmica of 5.6 mm²/s | |
Temperatura máx. de funcionamiento, largo | 0 - 1100 °C Show Material materials with Temperatura máx. de funcionamiento, largo of 0 - 1100 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 1E-6 - 1.04E-6 Ω·m Show Material materials with Resistividad eléctrica of 1E-6 - 1.04E-6 Ω·m |
100.0 °C | 1.07E-6 Ω·m Show Material materials with Resistividad eléctrica of 1.07E-6 Ω·m | |
200.0 °C | 1.11E-6 Ω·m Show Material materials with Resistividad eléctrica of 1.11E-6 Ω·m | |
300.0 °C | 1.14E-6 Ω·m Show Material materials with Resistividad eléctrica of 1.14E-6 Ω·m | |
400.0 °C | 1.17E-6 Ω·m Show Material materials with Resistividad eléctrica of 1.17E-6 Ω·m | |
500.0 °C | 1.19E-6 Ω·m Show Material materials with Resistividad eléctrica of 1.19E-6 Ω·m | |
600.0 °C | 1.22E-6 Ω·m Show Material materials with Resistividad eléctrica of 1.22E-6 Ω·m | |
700.0 °C | 1.23E-6 Ω·m Show Material materials with Resistividad eléctrica of 1.23E-6 Ω·m | |
800.0 °C | 1.25E-6 Ω·m Show Material materials with Resistividad eléctrica of 1.25E-6 Ω·m | |
900.0 °C | 1.57E-6 Ω·m Show Material materials with Resistividad eléctrica of 1.57E-6 Ω·m | |
1000.0 °C | 1.29E-6 Ω·m Show Material materials with Resistividad eléctrica of 1.29E-6 Ω·m | |
Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.15 % Show Material materials with Carbono of 0.15 % |
Cromo | 15 - 17 % Show Material materials with Cromo of 15 - 17 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Manganeso | 2 % Show Material materials with Manganeso of 2 % |
Nitrógeno | 0.11 % Show Material materials with Nitrógeno of 0.11 % |
Níquel | 33 - 37 % Show Material materials with Níquel of 33 - 37 % |
Silicona | 1 - 2 % Show Material materials with Silicona of 1 - 2 % |