Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00Wrought Copper High Copper Alloy
ASTM B194 Grade C17200 TD04Acero inoxidable austenítico
Sandvik 253 MASuministrada por:
Alleima (formerly Sandvik Materials Technology)Wrought Copper High Copper Alloy
ASTM B768 Grade C17510 TH04Wrought Copper High Copper Alloy
EN 1652 Grade C17200 TF00Nickel Chromium Iron Alloy
Sanicro 31HTSuministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable austenítico
Sandvik 2RE10Suministrada por:
Alleima (formerly Sandvik Materials Technology)Nickel Chromium Iron Alloy
Sanicro® 61Suministrada por:
Alleima (formerly Sandvik Materials Technology)Nickel Chromium Iron Alloy
EN 10095 Grade NiCr28FeSiCe solution annealed (+AT)Nickel Chromium Alloy
DIN 17742 Grade NiCr8020 solution annealed (+AT)Nickel Chromium Alloy
DIN 17742 Grade NiCr7030 solution annealed (+AT)Nickel Chromium Iron Alloy
DIN 17742 Grade NiCr6015 solution annealed (+AT)Nickel Chromium Alloy
DIN 17744 Grade NiCr22Mo7Cu solution annealed (+AT)Nickel Chromium Alloy
DIN 17744 Grade NiCr22Mo6Cu