Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.85 g/cm³ Show Material materials with Densidad of 7.85 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Nickel Steel |
Elongación | 20.0 °C | 24 % Show Material materials with Elongación of 24 % | |
Límite elástico Rp 0,2 | 20.0 °C | 280 MPa Show Material materials with Límite elástico Rp 0,2 of 280 MPa | |
Módulo de cizallamiento | 23.0 °C | 76 GPa Show Material materials with Módulo de cizallamiento of 76 GPa | Typical for Nickel Steel |
Módulo elástico | 23.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Nickel Steel |
Resistencia a la tracción | 20.0 °C | 480 - 630 MPa Show Material materials with Resistencia a la tracción of 480 - 630 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 460 J/(kg·K) Show Material materials with Calor específico of 460 J/(kg·K) | |
Coeficiente de dilatación térmica | 100.0 °C | 1.18E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.18E-5 1/K | |
300.0 °C | 1.24E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.24E-5 1/K | ||
500.0 °C | 1.36E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.36E-5 1/K | ||
Conductividad térmica | 50.0 °C | 36 W/(m·K) Show Material materials with Conductividad térmica of 36 W/(m·K) | |
Temperatura de fusión | 1316 - 1595 °C Show Material materials with Temperatura de fusión of 1316 - 1595 °C | Typical for Nickel Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.06 - 0.12 % Show Material materials with Carbono of 0.06 - 0.12 % |
Cobre | 0.3 % Show Material materials with Cobre of 0.3 % |
Cromo | 0.3 % Show Material materials with Cromo of 0.3 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Manganeso | 0.5 - 0.8 % Show Material materials with Manganeso of 0.5 - 0.8 % |
Molibdeno | 0.2 % Show Material materials with Molibdeno of 0.2 % |
Níquel | 2 - 3 % Show Material materials with Níquel of 2 - 3 % |
Silicona | 0.6 % Show Material materials with Silicona of 0.6 % |
Vanadio | 0.05 % Show Material materials with Vanadio of 0.05 % |